Embodiment 1
[0017] 1) Prepare co-solvent by volume: 2 parts of toluene, 4 parts of aromatic oil, 2 parts of n-butanol, 2 parts of iso-octanol;
[0018] 2) Prepare combustion accelerant by volume: 1 part of ethyl tert-butyl ether and 4 parts of methyl tert-butyl ether;
[0019] 3) Prepare metal corrosion inhibitors by volume: 1 part of benzotriazole, 2 parts of organic amine and 1 part of passivator;
[0020] 4) Prepare rubber swelling inhibitor by volume: 1 part of ferrocene and 0.5 part of ethyl acetate;
[0021] 5) First add 60 parts by volume of gasoline, 10 parts by volume of ethanol, 3 parts by volume of methanol, 10 parts by volume of co-solvent and 3 parts by volume of sorbitan palmitate into the raw material tank, and then add 5 parts by volume of combustion aid after mixing for 30 minutes Agent, 6 parts by volume of metal corrosion inhibitor, 2 parts by volume of rubber swelling inhibitor, stirred evenly at normal temperature and pressure, then pressurized to 70MPa, stirred for ...
Embodiment 2
[0023] 1) Prepare co-solvent by volume: 4 parts of toluene, 8 parts of aromatic oil, 5 parts of n-butanol, 3 parts of iso-octanol;
[0024] 2) Prepare combustion accelerant by volume: 5 parts of ethyl tert-butyl ether and 6 parts of methyl tert-butyl ether;
[0025] 3) Prepare metal corrosion inhibitors by volume: 5 parts of benzotriazole, 4 parts of organic amine and 3 parts of passivating agent;
[0026] 4) Prepare rubber swelling inhibitor by volume: 4 parts of ferrocene and 3 parts of ethyl acetate;
[0027] 5) First add 70 parts by volume of gasoline, 25 parts by volume of ethanol, 6 parts by volume of methanol, 20 parts by volume of co-solvent and 8 parts by volume of sorbitan monooleate into the raw material tank, and then add 10 parts by volume after mixing for 40 minutes Combustion enhancer, 8 parts by volume of metal corrosion inhibitor, 5 parts by volume of rubber swelling inhibitor, stirred evenly at normal temperature and pressure, then pressurized to 90MPa, stir...
Embodiment 3
[0029] 1) Prepare co-solvent by volume: 3 parts of toluene, 6 parts of aromatic oil, 4 parts of n-butanol, 2.5 parts of iso-octanol group;
[0030] 2) Prepare combustion accelerant by volume: 3 parts of ethyl tert-butyl ether and 5 parts of methyl tert-butyl ether;
[0031] 3) Prepare metal corrosion inhibitors by volume: 3 parts of benzotriazole, 3 parts of organic amine and 2 parts of passivator;
[0032] 4) Prepare rubber swelling inhibitor by volume: 3 parts of ferrocene and 2 parts of ethyl acetate;
[0033] 5) First, add 65 parts by volume of gasoline, 15 parts by volume of ethanol, 5 parts by volume of methanol, 15 parts by volume of co-solvent and 6 parts by volume of sorbitan monostearate into the raw material tank, and then add 8 volume parts after mixing for 35 minutes 1 part combustion enhancer, 7 parts by volume of metal corrosion inhibitor, 4 parts by volume of rubber swelling inhibitor, stirred evenly at normal temperature and pressure, then pressurized to 80MP...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com