Method for improving stability of carbon dioxide detection reagent
A technology for detecting reagents and carbon dioxide, applied in the field of carbon dioxide detection reagent protective film composition, to achieve the effect of improving stability and excellent stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Accurately weigh 5g of glycerin and 0.8g of ethylene glycol, and then dissolve them in 100ML of carbon dioxide detection reagent according to the above weighing sequence, then use 1mol / l hydrochloric acid or sodium hydroxide to adjust the pH to 8.0, and then add 10g of simethicone, A film composition composed of 9 g of light paraffin oil and Tween-205 g is added to the surface of the liquid, so that it spreads on the surface of the liquid to form a connected protective film. For the carbon dioxide detection kit used in the carbon dioxide protective film composition prepared above, the performance of the reagent is still good after the reagent is opened and placed in the reagent compartment for more than 30 days.
Embodiment 2
[0018] Accurately weigh 0.5g of polyoxyethylene lauryl ether and 3.5g of glycerin, and then dissolve it in 100ML of carbon dioxide detection reagent according to the above weighing sequence, then use 1mol / l hydrochloric acid or sodium hydroxide to adjust its pH to 8.0, and then add dimethyl A film composition composed of 10g of silicone oil, 5g of mineral oil and 205g of Tween is added to the surface of the liquid so that it spreads on the surface of the liquid to form a connected protective film. For the carbon dioxide detection kit used in the carbon dioxide protective film composition prepared above, the performance of the reagent is still good after the reagent is opened and placed in the reagent compartment for more than 30 days.
Embodiment 3
[0020] Accurately weigh 0.1g of glycerin and 20g of ethylene glycol, and then dissolve them in 100ML of carbon dioxide detection reagent according to the above weighing sequence, then use 1mol / l hydrochloric acid or sodium hydroxide to adjust the pH to 6.5, and then add 90g of simethicone, A film composition consisting of 0.1 g of light paraffin oil and 200.1 g of Tween is added to the surface of the liquid so that it spreads on the surface of the liquid to form a connected protective film. Place the treated carbon dioxide detection reagent in the reagent compartment, and the performance is still good after more than 30 days.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com