A kind of preparation method of iron ion exchange modified molecular sieve
A molecular sieve and iron ion technology, which is applied in the field of preparation of iron ion exchange modified molecular sieves, can solve the problems of repeated ferrous ions being easily oxidized in the liquid phase and low exchange degree, and achieve high exchange degree and easy operation. Simple, easy-to-remove effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] Reduced iron powder and HY parent molecular sieve with a silicon-aluminum ratio of 8 are mixed at a mass ratio of 1:1, and 1mol / L FeCl is added to the mixture of iron powder and parent molecular sieve 2 In the solution, add 1g of solid per 10ml of solution; stir at 80°C for 24 hours for ion exchange; after the exchange is completed, filter with suction and wash with deionized water; dry the sample at 110°C; place the sample in a magnetic field for magnetic separation Iron powder is extracted to obtain iron ion exchange modified molecular sieve.
Embodiment 2
[0040] Mix reduced iron powder with HZSM-5 parent molecular sieve with a silicon-aluminum ratio of 25 at a mass ratio of 1:1, and add 0.5mol / L FeCl to the mixture of iron powder and parent molecular sieve 2 In the solution, the solid-to-liquid ratio is 1g of solid per 10ml of solution; stir at 80°C for 24 hours for ion exchange; after the exchange is completed, filter with suction and wash with deionized water; dry the sample at 110°C; place the sample in Magnetic field, magnetically separate iron powder to obtain iron ion exchange modified molecular sieve.
Embodiment 3
[0042] Reduced iron powder and HY parent molecular sieve with a silicon-aluminum ratio of 5 are mixed at a mass ratio of 1:2, and the mixture of iron powder and parent molecular sieve is added with 0.3mol / L FeCl 2 In the solution, the solid-to-liquid ratio is 1g of solid per 10ml of solution; stir at 80°C for 12 hours for ion exchange; after the exchange, centrifuge and wash with deionized water; dry the sample at 150°C; place the sample in Magnetic field, magnetically separate iron powder to obtain iron ion exchange modified molecular sieve.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com