Embodiment 1
[0028] Each component is calculated in parts by weight: after heating 0.15 parts of ricinoleic acid to 90° C., adding a concentration of 30% NaOH solution, the amount of ricinoleic acid, octadecenoic acid and citric acid in subsequent steps can be Complete saponification is appropriate; then add 0.5 parts of cis-9-octadecenoic acid and 0.05 parts of citric acid, stir and mix and heat to melt and saponify, saponification time is 2 hours; after saponification is completed, add 4-ethyl-6- Propyl nonanol (C14 higher alcohol) higher alcohol 0.3 parts, prepared normal temperature phosphate rock flotation collector.
[0029] Using phosphate rock collector, flotation in a neutral environment at 10°C, positive flotation P 2 o 5 Phosphate rock with a grade of 21.25% and low grade can obtain phosphorous concentrate P 2 o 5 The grade is 32.12%, and the recovery rate is 85.02%, which is a good indicator.
Embodiment 2
[0031] The components are calculated in parts by weight: after heating 0.18 parts of ricinoleic acid to 100°C, adding a concentration of 35% KOH solution, the amount of which can be obtained in subsequent steps by ricinoleic acid, octadecenoic acid and citric acid It is advisable to completely saponify; then add 0.55 parts of trans-9-octadecenoic acid and 0.08 parts of citric acid, stir and mix and heat to melt and saponify. The saponification time is 2.5 hours; after saponification is completed, add 3-diethyl-5 - 0.19 parts of propyl heptanol (C15 higher alcohol) to prepare a normal temperature phosphate rock flotation collector.
[0032] Using this new type of phosphate rock collector, flotation in a neutral environment at 25°C, positive flotation of P 2 o 5 Phosphate rock with a grade of 21.25% and low grade can obtain phosphorous concentrate P 2 o 5 The grade is 32.55%, and the recovery rate is 85.10%, which is a good indicator.
Embodiment 3
[0034] Each component is calculated in parts by weight: after heating 0.2 parts of ricinoleic acid to 110° C., adding a concentration of 40% NaOH solution, the amount of ricinoleic acid, octadecenoic acid and citric acid in subsequent steps can be Complete saponification is appropriate; then add 0.6 parts of octadec-6-enoic acid and 0.1 parts of citric acid, stir and mix and heat to melt and saponify, saponification time is 3 hours; after saponification is completed, add 2,4-tetramethyl- 0.1 part of 5-diethyl octanol (C16 higher alcohol) was used to prepare a normal temperature phosphate rock flotation collector; the octadecenoic acid used came from waste oil extraction.
[0035] Using this new type of phosphate rock collector, flotation in a neutral environment at 35°C, positive flotation of P 2 o 5 Phosphate rock with a grade of 21.25% and low grade can obtain phosphorous concentrate P 2 o 5 The grade is 33.68%, and the recovery rate is 85.22%, which is a good indicator. ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com