An active and environmentally friendly technology, applied in the field of construction adhesives, can solve the problems that acrylamide is easily volatilized into the air, the quality is greatly affected by the formulation process, and the health of workers is affected, so as to protect personal health, avoid cancer risks, and facilitate promotion. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] The environmentally friendly construction active glue is made from the following raw materials in parts by weight: 60 parts of polyvinyl alcohol powder and 200 parts of ozone water.
[0012] The content percentage of ozone in the above-mentioned ozone water is 50%.
[0013] The preparation method of the above-mentioned environmentally friendly building active glue is: 10kg of tap water is placed in a stainless steel bucket, then the air stone is placed on the bottom of the stainless steel bucket, ozone is passed into the tap water by an ozone machine, and the ozone time is 40 minutes. After the introduction of ozone is completed, ozone water is obtained. After the ozone water is obtained, 2kg of polyvinyl alcohol powder is dissolved into the ozone water, and the mixture of polyvinyl alcohol powder and ozone water is stirred for 20 minutes. After the stirring is completed, That is, an environmentally friendly construction active glue is obtained.
Embodiment 2
[0015] The environmentally friendly construction active glue is made from the following raw materials in parts by weight: 100 parts of polyvinyl alcohol powder and 300 parts of ozone water.
[0016] The content percentage of ozone in the above-mentioned ozone water is 80%.
[0017] The preparation method of the above-mentioned environmentally friendly building active glue is: 20kg of tap water is placed in a stainless steel bucket, then the air stone is placed on the bottom of the stainless steel bucket, ozone is passed into the tap water by an ozone machine, and the ozone time is 60 minutes. After the introduction of ozone is completed, ozone water is obtained. After the ozone water is obtained, 4kg of polyvinyl alcohol powder is dissolved in the ozone water, and then the mixture of polyvinyl alcohol powder and ozone water is stirred for 40 minutes. After the stirring is completed, That is, an environmentally friendly construction active glue is obtained.
Embodiment 3
[0019] The environmentally friendly construction active glue is made from the following raw materials in parts by weight: 80 parts of polyvinyl alcohol powder and 250 parts of ozone water.
[0020] The content percentage of ozone in the above-mentioned ozone water is 75%.
[0021] The preparation method of the above-mentioned environmentally friendly building active glue is: 15kg of tap water is placed in a stainless steel bucket, then the air stone is placed on the bottom of the stainless steel bucket, ozone is passed into the tap water by an ozone machine, and the ozone time is 50 minutes. After the introduction of ozone is completed, ozone water is obtained. After the ozone water is obtained, 3kg of polyvinyl alcohol powder is dissolved in the ozone water, and then the mixture of polyvinyl alcohol powder and ozone water is stirred for 30 minutes. After the stirring is completed, That is, an environmentally friendly construction active glue is obtained.
[0022] The role of...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com