Rust glaze and method for making product thereof
A technology of rust and glaze, applied in the production field of rust glaze and its products, to achieve the effect of quiet and elegant decoration, vigorous momentum and convenient firing process control
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] Glaze preparation:
[0029] Get 22 parts by weight of albite, 5 parts by weight of calcium carbonate, 3 parts by weight of titanium dioxide, 20 parts by weight of kaolin, 5 parts by weight of quartz, 8 parts by weight of iron oxide, 20 parts by weight of manganese dioxide and 17 parts by weight of boron block; add water 110 parts by weight, ground into a glaze slurry in a ball mill, and the glaze slurry is passed through a 250-mesh or finer sieve for use; the steps of grinding into a glaze slurry include weighing raw materials, putting into a ball mill jar, adding water, sealing the lid, grinding, and opening the jar lid , release the glaze water, filter, adjust the concentration;
[0030] Product preparation:
[0031] Follow the steps below;
[0032] Blank making, bisque firing at 800°C for 4 to 5 hours, then naturally cool for later use;
[0033] Glazing, the glaze is made by biscuit firing into the porcelain body according to the conventional method, and the glaze...
Embodiment 2
[0040] The process is the same as in Example 1, except that the composition of the glaze slurry is different. The glaze composition of this example is: get 12 parts by weight of albite feldspar, 3 parts by weight of calcium carbonate, 2 parts by weight of titanium dioxide, 15 parts by weight of kaolin, 3 parts by weight of quartz, 7 parts by weight of iron oxide, 15 parts by weight of manganese dioxide and boron Melt 43 parts by weight; add 110 parts by weight of water, grind in a ball mill to form a glaze slurry for later use.
Embodiment 3
[0042] The process is the same as in Example 1, except that the composition of the glaze slurry is different. The glaze composition of this example is: get 26 parts by weight of albite, 8 parts by weight of calcium carbonate, 5 parts by weight of titanium dioxide, 20 parts by weight of kaolin, 6 parts by weight of quartz, 10 parts by weight of iron oxide, 22 parts by weight of manganese dioxide and boron 3 parts by weight of melt block; add 110 parts by weight of water, and grind into a glaze slurry in a ball mill for later use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com