[0105] The invention relates to a preparation method of a supported non-metallocene catalyst, comprising the following steps: dissolving a magnesium compound in a solvent to obtain a magnesium compound solution; making a porous carrier optionally subjected to thermal activation treatment and the magnesium compound solution contacting to obtain a first mixed slurry; contacting the non-metallocene complex with the first mixed slurry to obtain a second mixed slurry; directly drying the second mixed slurry to obtain a modified composite carrier, and A step of reacting a chemical treatment agent selected from group IVB metal compounds with the modified composite carrier to obtain the supported non-metallocene catalyst.
[0106] The magnesium compound will be specifically described below.
[0107] According to the present invention, the term "magnesium compound" refers to an organic or inorganic solid anhydrous magnesium-containing compound conventionally used as a carrier of a supp...
Embodiment 1
[0334] The magnesium compound is anhydrous magnesium chloride, the solvent is tetrahydrofuran, and the porous carrier is silicon dioxide, that is, silica gel, the model is ES757 from Ineos Company. Before use, the silica gel is continuously calcined at 600° C. under nitrogen atmosphere for 4 hours to be thermally activated. The non-metallocene complex adopts the structure The compound, the chemical treatment agent of the IVB group metal compound adopts titanium tetrachloride, and the solvent for the chemical treatment agent adopts hexane.
[0335]Weigh 5g of anhydrous magnesium chloride, add a solvent and dissolve it completely at normal temperature to obtain a magnesium compound solution, then add heat-activated silica gel, stir at normal temperature for 2 hours to form the first mixed slurry, then add a non-metallocene complex to obtain the second 2. Mix the slurry, then stir and react at room temperature for 6 hours, and dry in vacuum at room temperature to obtain a modifi...
Embodiment 1-1
[0340] Basically the same as Example 1, but with the following changes:
[0341] The porous carrier was changed to Grace's 955, and it was continuously calcined at 400° C. for 8 hours under a nitrogen atmosphere to be thermally activated.
[0342] The solvent is changed to toluene, and the non-metallocene complex adopts The chemical treatment agent for Group IVB metal compounds was changed to zirconium tetrachloride (ZrCl 4 ), the chemical treatment agent was changed to cyclohexane with a solvent.
[0343] Wherein the ratio is as follows: the ratio of magnesium compound to solvent is 1mol: 150ml; the molar ratio of magnesium compound to non-metallocene complex is 1: 0.15; the mass ratio of magnesium compound to porous carrier is 1: 4; the ratio of magnesium compound to IVB group The molar ratio of the chemical treatment agent in terms of metal elements is 1:0.20.
[0344] Supported non-metallocene catalysts are designated CAT-1-1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com