Water-based PU wiping-coke treating agent for synthetic leather and its preparation method
A synthetic leather and treatment agent technology, which is applied in fiber treatment, textiles and papermaking, etc., can solve the problems of synthetic leather bottom layer dissolution, flammability, and poor comprehensive effect of synthetic leather, and achieve the effect of increasing production cost and convenient material selection
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] The water-based PU scorching treatment agent for synthetic leather consists of 20 parts by weight of water-based polyurethane resin varnish, 5 parts by weight of modified polyurethane emulsion, 30 parts by weight of water, 10 parts by weight of water-based silicone oil, 7 parts by weight of modified polyamide wax powder, and 3 parts by weight It consists of 1 part by weight of silica matting powder, 1 part by weight of silicone leveling agent, 2 parts by weight of silicone defoamer and 2 parts by weight of water-based polyurethane thickener.
[0029] The preparation method of the above-mentioned water-based PU scorching treatment agent for synthetic leather is: under normal temperature and pressure, 20 parts by weight of water-based polyurethane resin varnish, 5 parts by weight of modified polyurethane emulsion, 3 parts by weight of silica matting powder, 10 parts by weight of Parts of water-based silicone oil, 7 parts by weight of modified polyamide wax powder, 2 parts ...
Embodiment 2
[0032] The water-based PU scorching treatment agent for synthetic leather consists of 25 parts by weight of water-based polyurethane resin varnish, 10 parts by weight of modified polyurethane emulsion, 40 parts by weight of water, 12 parts by weight of water-based silicone oil, 5 parts by weight of modified polyamide wax powder, 2 parts by weight It consists of a silicon dioxide matting powder, 0.5 parts by weight of a silicone leveling agent, 5 parts by weight of a silicone defoamer and 0.5 parts by weight of a water-based polyurethane thickener.
[0033] The preparation method of the above-mentioned water-based PU scorching treatment agent for synthetic leather is: under normal temperature and pressure, 25 parts by weight of water-based polyurethane resin varnish, 10 parts by weight of modified polyurethane emulsion, 2 parts by weight of silica matting powder, 12 parts by weight Parts of water-based silicone oil, 5 parts by weight of modified polyamide wax powder, 5 parts by ...
Embodiment 3
[0036] The water-based PU scorching treatment agent for synthetic leather consists of 23 parts by weight of water-based polyurethane resin varnish, 7 parts by weight of modified polyurethane emulsion, 35 parts by weight of water, 11 parts by weight of water-based silicone oil, 6 parts by weight of modified polyamide wax powder, and 2.5 parts by weight It consists of 0.8 parts by weight of silicon dioxide matting powder, 0.8 parts by weight of silicone leveling agent, 3.5 parts by weight of silicone defoamer and 1.8 parts by weight of water-based polyurethane thickener.
[0037] The preparation method of the above-mentioned water-based PU scorching treatment agent for synthetic leather is: under normal temperature and pressure, 23 parts by weight of water-based polyurethane resin varnish, 7 parts by weight of modified polyurethane emulsion, 2.5 parts by weight of silica matting powder, 11 parts by weight of Parts of water-based silicone oil, 6 parts by weight of modified polyami...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com