A drug-loaded nano-fiber mat technology, which is applied in the direction of pharmaceutical formulations, medical preparations of non-active ingredients, antipyretics, etc., can solve problems such as low safety, low encapsulation efficiency, and complicated technology, and achieves the goal of preparation methods Simple, easy-to-operate, easy-to-carry effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0037] Preparation of coaxial structure 1
[0038] (1) Preparation of spinning dope: Suspend 0.875g of ketoprofen in 10mL of absolute ethanol containing 3.5g of polyvinylpyrrolidone PVP K30, stir mechanically (12h) and continue heating (50±1°C, 8h), and prepare Spinning stock solution 1; suspend 0.6g ketoprofen in 10mL absolute ethanol containing 2.4g ethyl cellulose, mechanically stir (12h) and continue heating (50±1°C, 8h) to prepare spinning stock solution 2;
[0039] (2) Preparation of coaxial structure 1: Pour the prepared spinning stock solutions 1 and 2 into the solution reservoirs 1 and 2 (5mL syringes) respectively, connect the flattened No. 7 injection needles, and then connect the two needles to On the coaxial device (the polyvinylpyrrolidone spinning solution is the outer layer, and the ethyl cellulose spinning solution is the inner layer), the device is connected to the positive pole of the high-voltage power supply, and the aluminum foil fiber receiving plate wi...
Embodiment 2
[0041] Preparation of coaxial structures 2
[0042] (1) Preparation of spinning dope: Suspend 0.875g of ketoprofen in 10mL of absolute ethanol containing 3.5g of polyvinylpyrrolidone PVP K30, stir mechanically (12h) and continue heating (50±1°C, 8h), and prepare Spinning stock solution 1; suspend 0.6g ketoprofen in 10mL absolute ethanol containing 2.4g ethyl cellulose, mechanically stir (12h) and continue heating (50±1°C, 8h) to prepare spinning stock solution 2;
[0043] (2) Preparation of coaxial structure 2: Pour the prepared spinning stock solutions 1 and 2 into the solution reservoirs 1 and 2 (5mL syringes) respectively, connect the flattened No. 7 injection needles, and then connect the two needles to the On the coaxial device (the ethyl cellulose spinning solution is the outer layer, and the polyvinylpyrrolidone spinning solution is the inner layer), the device is connected to the positive pole of the high-voltage power supply, and the aluminum foil fiber receiving pla...
Embodiment 3
[0045] Preparation of multi-layer coaxial drug-loaded fiber mats
[0046] (1) Preparation of spinning dope: Suspend 0.875g of ketoprofen in 10mL of absolute ethanol containing 3.5g of polyvinylpyrrolidone PVPK30, stir mechanically (12h) and continue heating (50±1°C, 8h) to prepare Spinning stock solution 1; suspend 0.6g ketoprofen in 10mL absolute ethanol containing 2.4g ethyl cellulose, mechanically stir (12h) and continue heating (50±1°C, 8h) to make spinning stock solution 2;
[0047] (2) Preparation of multi-layer coaxial structure drug-loaded fiber mat:
[0048] Electrospinning of coaxial structure 1 (first and second layer electrospinning): Pour the above-mentioned prepared spinning stock solutions 1 and 2 into solution reservoirs 1 and 2 (5mL syringes), respectively, and connect the flattened No. 7 injection Needles, two needles are connected to the coaxial device (polyvinylpyrrolidone spinning solution is the outer layer, ethyl cellulose spinning solution is the inne...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com