Process for surfacing stainless steel sealing face on ductile cast iron valve base
A technology of ductile iron and stainless steel, which is used in manufacturing tools, welding equipment, metal processing, etc., can solve the problems of unstable quality, difficult quality assurance, low deposition rate, etc., and achieves a wide range of applicable temperatures and high utilization rate of welding materials. , the effect of strong heat resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] The valve base is ductile iron QT450-10, and 308 stainless steel solid core welding wire is surfacing with pulse melting electrode gas shielded welding:
[0022] Pulse MIG shielded welding, the joint type is flat surfacing welding, the wire diameter is φ1.2, the minimum thickness of the welding layer is 3mm, single-layer welding, the minimum preheating temperature is 100°C, and the shielding gas is 97% argon +3 % carbon dioxide mixed gas, the mixed gas flow rate is 20-22L / min, the current is pulse direct current (DC) 145A, the polarity is negative polarity, the metal transition method is jet transition, swing welding, single pass welding, and the specification of the contact tip is φ1. 4. The welding speed is 11-12cm / min, and the temperature is kept at 370±10℃ for 2 hours after welding.
Embodiment 2
[0024] The valve base is ductile iron QT500-7, and SUS 316 stainless steel solid wire is surfacing with pulse melting electrode gas shielded welding:
[0025] Pulse MIG shielded welding, the joint type is flat surfacing welding, the diameter of the welding wire is Φ1.2, the minimum thickness of the welding layer is 5mm, two-layer welding, the minimum preheating temperature is 150°C, and the shielding gas is 98% argon+ 2% carbon dioxide mixed gas, the mixed gas flow rate is 20-22L / min, the current is pulsed direct current (DC) 150A, the polarity is negative polarity, the metal transition method is jet transition, swing welding, single pass welding, and the specification of the contact tip is Φ1 .4. The welding speed is 11-12cm / min, and the temperature is kept at 400±10℃ for at least 2 hours after welding.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com