Method for producing granular potassium sulfate
A production method and technology of potassium sulfate, applied in the directions of potash fertilizers, fertilizer mixtures, inorganic fertilizers, etc., can solve the problems of nutrient distribution ratio limitation, etc., and achieve the effects of low production cost, short technological process and smooth surface.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment approach
[0016] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENT: The process of the present invention is described through the following examples. However, the examples do not limit the invention.
example 1
[0018] Preparation of binder: Add 420 parts of water into the jacketed reactor, start stirring, heat to 70°C, add 45 parts of polyvinyl alcohol under stirring, heat up to 90°C, keep warm until the polyvinyl alcohol is completely dissolved into a transparent solution . Then cool the solution down to 50°C, add 1 part of polyoxyethylene castor oil, continue to add 0.5 part of polyoxyethylene octylphenol ether and 1 part of dibutyl phthalate, maintain 50°C, stir for 30 minutes, and cool down To 30°C, slowly add 70 parts of sodium silicate under rapid stirring, after the addition is complete, keep at 40°C, continue to stir and react for 0.5 hours, and then discharge to obtain the binder.
[0019] This example is batch production. Add 1,000 kg of powdered potassium sulfate with a fineness of less than 60 meshes to the disc granulator, spray 10 kg of the above prepared binder, and rotate and granulate into balls in the disc granulator. After drying, cooling and sieving, 910 kg of g...
example 2
[0021] Preparation of binder: Add 500 parts of water into the jacketed reactor, start stirring, heat to 70°C, add 40 parts of polyvinyl alcohol under stirring, heat up to 90°C, keep warm until the polyvinyl alcohol is completely dissolved into a transparent solution . Then cool the solution down to 50°C, add 0.2 parts of polyoxyethylene castor oil, continue to add 0.4 parts of polyoxyethylene octylphenol ether and 0.6 parts of dibutyl phthalate, maintain 50°C, stir for 30 minutes, and cool down To 30°C, slowly add 60 parts of sodium silicate under rapid stirring, after the addition, keep at 40°C, continue to stir and react for 0.5 hours, and then discharge the material to obtain the binder.
[0022] This example is for continuous production. Add the powdered potassium sulfate with a fineness of less than 60 mesh into the drum granulator at 1000 kg / hour, spray the above-mentioned binder at 40 kg / hour, and granulate into balls in the drum granulator . After drying, cooling an...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com