Preparation method of nano-grade layered silver-carrying-amino acid complex antibacterial agent
A nano-layered, amino acid technology, applied in botany equipment and methods, animal repellants, plant growth regulators, etc., can solve the problems of easy discoloration, slow-release performance and salt tolerance, and low silver loading. Achieve the effect of improved antibacterial activity, good anti-discoloration performance, and simple raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] Embodiment 1: A kind of preparation method of nano-layered silver-loaded amino acid antibacterial agent
[0028] Add 9.6mL each of 250mM silver nitrate and 250mM histidine solution into a 100mL beaker, add 80.8mL deionized water, the total volume of the solution is 100mL, mix well, place at room temperature for 30min, stir in a water bath at 50°C for 15min, and the stirring speed is 800r / min, add 1.0 g of high-purity montmorillonite, stir evenly, seal, place in a 50°C water bath and continue stirring overnight, cool, and centrifuge, and dry the precipitate in a 60°C drying oven.
Embodiment 2
[0029] Embodiment 2: A kind of preparation method of nano-layered silver-loaded amino acid antibacterial agent
[0030] Add 9.6mL each of 250mM silver nitrate and 250mM histidine solution into a 100mL beaker, add 80.8mL deionized water, the total volume of the solution is 100mL, mix well, place at room temperature for 30min, stir in a water bath at 50°C for 15min, and the stirring speed is 800r / min, add 1.0 g of high-purity montmorillonite, stir evenly, seal, place in a 50°C water bath and continue stirring overnight, cool, and centrifuge, and dry the precipitate in a 70°C drying oven.
Embodiment 3
[0031] Embodiment 3: A kind of preparation method of nano-layered silver-loaded amino acid antibacterial agent
[0032] Add 9.6mL each of 250mM silver nitrate and 250mM histidine solution into a 100mL beaker, add 80.8mL deionized water, the total volume of the solution is 100mL, mix well, place at room temperature for 30min, stir in a water bath at 50°C for 15min, and the stirring speed is 800r / min, add 1.0 g of high-purity montmorillonite, stir evenly, seal, place in a water bath at 50°C and continue stirring overnight, cool and centrifuge, and dry the precipitate at room temperature.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com