Method for preparing polyurethane foam from curcas oil base rigid foam polyether
A technology of polyurethane foam and jatropha oil, applied in the field of molecular polymerization, can solve the problem of high price, and achieve the effects of low cost, good compatibility and cost reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Add jatropha oil 1000g, 180 diethylene glycol, and 4g sodium hydroxide in a 2L glass kettle, stir and heat up to 170 degrees, react for 3 hours, detect the hydroxyl value, and discharge.
[0024] Modified jatropha oil A hydroxyl value: 126mgKOH / g
Embodiment 2
[0026] Add jatropha oil 1000g, 140 g of pentaerythritol, 5 g of potassium hydroxide in a 2L glass kettle, stir and heat up to 170 degrees, react for 3 hours, detect the hydroxyl value, and discharge.
[0027] Modified jatropha oil B hydroxyl value: 199mgKOH / g
Embodiment 3
[0029] Add jatropha oil 1000g, 160 g of triethanolamine, 6 g of calcium hydroxide in a 2L glass kettle, stir and heat up to 170 degrees, react for 3 hours, detect the hydroxyl value, and discharge.
[0030] Modified jatropha oil C hydroxyl value: 231mgKOH / g
PUM
Property | Measurement | Unit |
---|---|---|
hydroxyl value | aaaaa | aaaaa |
hydroxyl value | aaaaa | aaaaa |
hydroxyl value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com