Method for preparing titanium product
A product, a technology of pure titanium, applied in the field of preparation of titanium products, can solve problems such as difficult-to-process structures and complex precision parts, and achieve the effects of reducing energy consumption and cost, saving technological processes, and net-shaped products
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Put the pure titanium powder with an average particle diameter of 5 microns on the platform of the laser sintering equipment. The object is deconstructed into a two-dimensional plane with a layer thickness of 30 microns, and the layer thickness of the powder laying is controlled at 30 microns for sintering. Subsequently, the sintered pure titanium sample was vacuum annealed, and the vacuum degree was controlled at 1X10 -3 ~1X10 -6 Pa, the temperature is 580°C, and the holding time is 1 hour, and finally a pure titanium product with high precision and complex structure is obtained.
Embodiment 2
[0018] Put the Ti-6Al-4V alloy powder with an average particle diameter of about 10 microns on the platform of the laser sintering equipment, the sintering atmosphere is argon protection, the laser spot is controlled at 80 microns, and the line scanning speed is controlled at 3 m / In seconds, the laser sintered object is deconstructed into a two-dimensional plane with a layer thickness of 40 microns, and the layer thickness of the powder laying is controlled at 40 microns for sintering. Subsequently, the sintered Ti-6Al-4V sample was annealed under atmosphere protection. The protection atmosphere was argon, the temperature was 650°C, and the holding time was 2 hours. Finally, Ti-6Al-4V with high precision and complex structure was obtained. 4V products.
Embodiment 3
[0020] Put the Ti-5Al-3V alloy powder with an average particle diameter of about 0.5 microns on the platform of the laser sintering equipment, the sintering atmosphere is argon protection, the laser spot is controlled at 40 microns, and the line scanning speed is controlled at 3 m / In seconds, the laser sintered object is deconstructed into a two-dimensional plane with a layer thickness of 20 microns, and the layer thickness of the powder laying is controlled at 20 microns for sintering. Subsequently, the sintered Ti-5Al-3V sample was annealed under atmosphere protection. The protection atmosphere was argon, the temperature was 650°C, and the holding time was 2 hours. Finally, Ti-5Al-3V with high precision and complex structure was obtained. 3V products.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com