Production method of nanometer antibiosis cashmere knit fabric
A production method and technology of knitted fabrics, which are applied in the field of production of nano-antibacterial cashmere knitted fabrics, to achieve the effects of odor removal, soft luster, and smooth handle
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] EGb / nano-silver composite antibacterial agent is dissolved in 30kg water (fabric water-bath ratio is 1: 20) by 8% (i.e. 120ml) of fabric weight and is fully mixed and dissolved, and is formulated into antibacterial finishing solution; then, 5 pieces of heavy 300g The bright blue cashmere knitted fabric is soaked in the prepared antibacterial finishing solution, kept at 50°C for 20 minutes and then dehydrated;
[0026] Then, immerse in the prepared adhesive solution (the amount of adhesive added is 8% of the dry weight of the fabric, and the water bath ratio of the fabric is 1:20), keep it at 40°C for 15 minutes and then dehydrate;
[0027] Then, immerse in the prepared cashmere softener solution (the amount of softener added is 2% of the dry weight of the fabric, and the fabric water bath ratio is 1:20), soak for 25 minutes at a water temperature of 40°C, and then pour it into the washing machine for 2 minutes. , and then, the finished product is dehydrated, dried and i...
Embodiment 2
[0031] EGb / nano-silver composite antibacterial agent is dissolved in 75kg water (fabric water-bath ratio is 1: 25) by 9% (i.e. 240ml) of fabric weight and fully mixes and dissolves, is deployed into antibacterial finishing solution, and 10 red cashmeres with a weight of 300g The knitted fabric is soaked in the prepared antibacterial finishing solution, kept at 53°C for 23 minutes and then dehydrated;
[0032] Immerse in the prepared adhesive solution (the amount of adhesive added is 8% of the dry weight of the fabric, and the water bath ratio of the fabric is 1:20), keep it at 42°C for 13 minutes, and then dehydrate;
[0033] Immerse in the prepared cashmere softener solution (the amount of softener added is 2% of the dry weight of the fabric, and the water-bath ratio of the fabric is 1:20), soak for 22 minutes at 42°C, then pour it into the washing machine for 3 minutes, and dehydrate it. , drying and ironing to get the finished product.
[0034] According to GB18401-2003 qu...
Embodiment 3
[0037] EGb / nano-silver composite antibacterial agent is dissolved in 90kg water (fabric water-bath ratio is 1: 20) by 10% (i.e. 360ml) of fabric weight and fully mixes and dissolves, is deployed into antibacterial finishing solution, and 15 gray cashmeres with a weight of 300g The knitted fabric is soaked in the prepared antibacterial finishing solution, kept at 55°C for 25 minutes and then dehydrated;
[0038] Immerse in the prepared adhesive solution (the amount of adhesive added is 8% of the dry weight of the fabric, and the water bath ratio of the fabric is 1:20), keep it at 40°C for 15 minutes, and then dehydrate;
[0039] Immerse in the prepared cashmere softener solution (the amount of softener added is 2% of the dry weight of the fabric, and the water-bath ratio of the fabric is 1:20), soak for 25 minutes at a water temperature of 40°C, then pour it into the washing machine for 5 minutes, and dehydrate it. , drying and ironing to get the finished product.
[0040]Acco...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com