Preparation method of chemical battery pole piece
A technology of chemical batteries and manufacturing methods, which is applied in the direction of electrode manufacturing, battery electrodes, circuits, etc., can solve the problems of difficult precise control of pressure, uneven force on the baseband, high material requirements, etc., and achieve good uniformity, easy force, and volume small effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] A preparation method of a chemical battery, comprising the steps of gluing 1, powdering 2, rolling 3, etc., first brushing slurry on a foamed nickel-based tape with a thickness of 0.95 mm, the slurry is made of 1 kg of water, bonding 0.35 kg of polytetrafluoroethylene as an agent and 0.05 kg of nickel powder as a conductive agent (if a certain concentration of polytetrafluoroethylene emulsion is used, the amount of water can be reduced accordingly), and then the active material and additives are powdered by the powder box. Brush the mixed powder into the base belt coated with slurry, and immediately enter the hydraulic horizontal roller machine for rolling. The top view of the horizontal rolling machine is as follows figure 1 As shown, it is composed of bearing 4, roller body 5, hydraulic motor 6, hydraulic cylinder 8, oil pipe 7, oil pump 9, etc. The diameter of the roller of the horizontal roller machine is φ800mm, and the tabletting parameters are as follows:
[0024...
Embodiment 2
[0027] First, the slurry is brushed on a foamed nickel-based belt with a thickness of 0.95 mm. The slurry is mixed with 1 kg of a mixed solvent of N-methylpyrrolidone and ethanol in any proportion, polyvinyl alcohol and polyvinylidene fluoride in any proportion to form a viscous material. 0.02 kg of contact powder, nickel powder and carbon powder are mixed in any proportion to form 0.1 kg of conductive agent mixed powder, and then the mixed powder of active substance and additive is rolled and pressed on the base tape coated with slurry through powder feeding box On the surface, spray one layer of the above-mentioned slurry on its surface, and immediately enter the hydraulic horizontal roller machine for rolling, and the result is the same as that of Example 1.
Embodiment 3
[0029] First, on the foamed nickel base belt with a thickness of 0.95mm, fill and press the powdery mixture composed of active substances and additives on the battery base belt by spraying; spray a paste-like material on the surface of the mixture, and in the paste-like material It contains a solvent and an adhesive, wherein the solvent is water and ethanol, the adhesive is polyvinyl alcohol, and the weight ratio of the solvent to the adhesive is 1:0.003. Immediately enter the hydraulic horizontal pair of rollers for rolling, and the result is the same as in Example 1.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com