[0168] The sealant composition of the present invention comprises a suitable elastomer, more specifically sodium polyacrylate, in suspension. Sodium polyacrylate in particulate form will pass through tire valves in this suspension without clogging.
[0169] This composition was prepared in two parts, hereinafter respectively referred to as premixed rosin solution (A) and granule solution (B), which were then mixed as explained below.
[0170] Premixed rosin solution (A) includes the following items (content is given in weight percent):
[0171] (1) Ethylene glycol-18;
[0172] (2) Propylene glycol-24;
[0173] (3) Water -15.8;
[0174] (4) ammonia water 20%-4.0;
[0175] (5) Ethanol-4.0;
[0176] (6) Formalin-0.2;
[0177] (7) Propylene Glycol-24.0 and
[0178] (8) Rosin - 10.0.
[0179] Solution (A) was formed as described below.
[0180] Components (1) to (6) are first mixed under stirring, preferably in descending order. Rosin (7) was added separately to the remai...
Embodiment 2
[0196] Another preferred embodiment relates to a method for the preparation of a composition for sealing punctures and pneumatic tires, said method comprising the steps of:
[0197]A. Form the hot phase premix by adding rosin (1.5% by weight of the final composition) and propylene glycol (1.5% by weight of the final composition) to a steam jacketed vessel and heating to a temperature of about 100°C Until the rosin is completely melted in propylene glycol, then cooled under stirring until a temperature of about 50°C is reached, then ethylene glycol (1.0% by weight of the final composition), 20% ammonia water (1.0% by weight of the final composition), 0.4% by weight), water (0.7% by weight of the final composition), polyethylene powder (10 μm to 180 μm in size) (1.0% by weight of the final composition), diatomaceous earth (0.8% by weight of the final composition ) and zinc stearate (accounting for 0.2% by weight of the final composition);
[0198] B. Form the gel phase premix i...
Embodiment 3
[0204] A composition for sealing a punctured vehicle tire, said composition comprising the following ingredients (all amounts are by weight percent of the final composition):
[0205] (1) Propylene glycol 81.0
[0206] (2) Glycerin 1.0
[0207] (3) Xanthan gum 0.11
[0208] (4) flax husk powder 0.012
[0209] (5) Carboxymethyl cellulose 0.03
[0210] (6) Diatomaceous earth 0.25
[0211] (7) Gum resin powder 1.35
[0212] (8) Magnesium carbonate 0.135
[0213] (9) Rice bran powder 0.3
[0214] (10) Titanium dioxide 0.075
[0215] (11) Cork powder 0.15
[0216] (12) Bark powder (dry) 0.1
[0217] (13) Asking powder 0.1
[0218] (14) Polyethylene powder 0.2
[0219] (15) Water 13.176
[0220] (16) Sodium bicarbonate 0.05
[0221] (17) Ammonium carbonate 0.05
[0222] (18) Sodium borate 1.0
[0223] (19) Formalin 0.2
[0224] (20) Fluorescein 0.012, and
[0225] (21) One or more polyacrylates in an amount of 0.05 to 2.0% by weight.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com