Sulphate-potassium magnesium fertilizer and preparation method thereof
A technology of potassium magnesium sulfate fertilizer and sulfate ion, which is applied in the direction of magnesium fertilizer, potash fertilizer, inorganic fertilizer, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A kind of potassium sulfate fertilizer, containing 10% of the sulfate radical soda-making waste residue and 90% of potassium layer stone powder, in the described soda-making waste residue, alkali slag accounts for 70%, calcium ion accounts for 30%, and magnesium ion accounts for 0%. The soda-making waste slag is obtained by rinsing, filtering and neutralizing the waste slag produced by the ammonia-soda method. There are 10% sulfate ions left in the waste slag. But when the magnesium ion content is zero, it can be prepared as potassium sulfate fertilizer.
[0026] The preparation method of the above-mentioned potassium magnesium sulfate fertilizer: firstly grind the natural potash stone into potash powder below 200 mesh; then mix the alkali-making waste residue and potash powder according to the above ratio; Carry out calcination, and the calcination time is 1 hour; cool to obtain the finished product.
Embodiment 2
[0028] A kind of potassium magnesium sulfate fertilizer, which contains 20% of the sulfate residue and 80% of the potassium layer stone powder. In the soda residue, the alkali residue accounts for 60%, the calcium ion accounts for 38%, and the magnesium ion accounts for 2%. The used soda residue is obtained by rinsing, filtering and neutralizing the waste residue produced by the ammonia-soda method, and 20% of sulfate ions remain in the waste residue.
[0029] The preparation method is the same as in Example 1, wherein the calcination temperature is 1200° C., and the calcination time is 0.5 hour.
Embodiment 3
[0031] A kind of potassium magnesium sulfate fertilizer, which contains 30% of sulfate root alkali-making waste residue and 70% of potassium layer stone powder. In the described alkali-making waste residue, alkali residue accounts for 45%, calcium ion accounts for 50%, and magnesium ion accounts for 5%. The used soda-making waste residue is obtained by rinsing, filtering and neutralizing the waste residue produced by ammonia-soda method, and 30% sulfate ion remains in the waste residue.
[0032] The preparation method is the same as in Example 1, wherein the calcination temperature is 1200° C., and the calcination time is 2 hours.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com