A technology for lubricants and chains, applied in the direction of lubricating compositions, etc., can solve the problems of poor hard water resistance, high solid content, and clogging of sprayers by scale, so as to prolong the service life, improve the workshop environment, and reduce the bottle pouring rate. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0045] (1) Mix 50g triethanolamine oleate and 60g triethanolamine, stir well, add 60g gluconoside and stir for 15 minutes, then add 30g LF-131, 20g isothiazolinone, 10g polymaleic acid, 10g benzene Piantriazole, 10g sodium xylene sulfonate were stirred for 30 minutes;
[0046] (2) Add 50g of EDTA-2Na into 700g of pure water, heat to 50°C and stir until it dissolves evenly;
[0047] (3) Mix the mixture obtained in the above two steps and stir evenly.
[0048] (4) Sealed and protected from light, diluted with industrial water at a ratio of 1:200 and sprayed for use.
Embodiment 2
[0050] (1) Mix 20g triethanolamine oleate and 30g triethanolamine, stir well, add 40g gluconoside and stir for 15 minutes, then add 10g LF-131, 10g isothiazolinone, 10g polymaleic acid, 10g benzene Piantriazole, 10g sodium xylene sulfonate were stirred for 30 minutes;
[0051] (2) Add 30g of EDTA-2Na into 650g of pure water, heat to 53°C and stir until it dissolves evenly;
[0052] (3) Mix the mixture obtained in the above two steps and stir evenly.
[0053] (4) Sealed and protected from light, diluted with industrial water at a ratio of 1:200 and sprayed for use.
Embodiment 3
[0055] (1) Mix 70g triethanolamine oleate and 90g triethanolamine, stir evenly, add 70g gluconoside and stir for 15 minutes, then add 30g LF-131, 20g isothiazolinone, 20g polymaleic acid, 20g benzene Piantriazole, 20g sodium xylene sulfonate were stirred for 30 minutes;
[0056] (2) Add 60g of EDTA-2Na into 750g of pure water, heat to 60°C and stir until it dissolves evenly;
[0057] (3) Mix the mixture obtained in the above two steps and stir evenly.
[0058] (4) Sealed and protected from light, diluted with industrial water at a ratio of 1:200 and sprayed for use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com