Fibre-reinforced anti-crack mortar dry powder
An anti-crack mortar and fiber-reinforced technology, applied in the field of special anti-crack mortar, can solve problems such as affecting the quality of the project and normal use, unfavorable material promotion and use, large shrinkage and deformation, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A fiber-reinforced anti-cracking mortar dry powder, its composition and weight content are: 42.5P.O cement 10%, fine sand 75%, silicon-aluminum hollow ball 12%, polyester fiber 1.48%, composed of expansion agent and air-entraining agent according to 0.5% mineral-type shrinkage inhibitor, 0.02% cement hydration regulator, and 1% modifier compounded at a weight ratio of 1000:1; wherein the composition of the hydration regulator and the weight percentage of the cement component are: glucose Sodium acid 0.2‰, paper mill sewage dried at 80°C 1‰; the composition and weight content of the modifier are: industrial grade vinyl acetate-ethylene copolymer 10%, heavy calcium powder and talcum powder 90%.
Embodiment 2
[0021] A fiber-reinforced anti-cracking mortar dry powder, its composition and weight content are: 42.5P.O cement 15%, fine sand 72%, silicon-aluminum hollow ball 9%, polypropylene fiber 2%, composed of expansion agent and air-entraining agent according to 0.78% of mineral type shrinkage inhibitor, 0.05% of cement hydration regulator, and 1.2% of modifier compounded at a weight ratio of 1000:1; the composition of the hydration regulator and the weight percentage of the cement components are: more Sodium polyphosphate 1‰, paper mill sewage dried at 80°C 1‰; modifier composition and weight content: industrial grade vinyl acetate homopolymer 12%, heavy calcium powder and talcum powder 88%.
Embodiment 3
[0023] A fiber-reinforced anti-cracking mortar dry powder, its composition and weight content are: 42.5P.O cement 20%, fine sand 70%, silicon-aluminum hollow ball 6.76%, polyester fiber 1%, composed of expansion agent and air-entraining agent according to 1% mineral type shrinkage inhibitor, 0.04% cement hydration regulator, and 1.2% modifier compounded at a weight ratio of 1000:1; the composition of the hydration regulator and the weight percentage of the cement components are: sucrose 0.5‰, paper mill sewage dried at 80°C 1.5‰; the composition and weight content of the modifier are: industrial grade polyethylene-vinyl acetate copolymer 15%, heavy calcium powder and talcum powder 85%.
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com