Coiled lead-acid battery with lead foam negative electrode grid and preparing method thereof
A lead-acid battery, lead foam technology, applied in the direction of lead-acid battery, lead-acid battery construction, electrode carrier/current collector, etc. , the high quality of the wound lead-acid battery, etc., to achieve the effect of high utilization of active materials, improved specific energy, and low battery quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0006] Specific implementation mode one: combine Figure 4 Describe this embodiment, in this embodiment, the lead-foamed negative electrode grid wound lead-acid battery includes a battery cover 1, a positive terminal 2, a pole ear 3, a mandrel 4, an outer circular fixture 8, a battery case 9, and a grid bottom Holder 10, exhaust valve 11, negative pole terminal 12, it also includes positive pole 7 surrounding mandrel 4, negative pole 5 with foamed lead negative pole grid as current collector and AGM separator 6 between positive pole 7 and negative pole 5.
specific Embodiment approach 2
[0007] Embodiment 2: The difference between this embodiment and Embodiment 1 is that the positive electrode 7 is a positive lead foil grid or a positive lead cloth grid coated with positive lead paste.
specific Embodiment approach 3
[0008] Specific embodiment three: the present embodiment realizes the preparation of the lead-foamed negative electrode grid wound lead-acid battery through the following steps: (1) and paste: prepare the positive lead paste coated with the positive electrode grid and the lead paste coated with the foamed lead negative electrode grid Negative electrode paste; (2) Pretreatment: Thin the foamed lead negative electrode grid to 0.6-1.1mm with a tablet press, then cut the thinned foamed lead negative electrode grid and positive electrode grid to the same size, and press The thin foamed lead negative grid is placed in a vacuum drying oven at 160-180°C for 1.8-2.2 hours; (3) Paste application: the positive electrode paste is evenly applied to the positive electrode grid to make the positive electrode, and the negative electrode paste is evenly applied to the The foamed lead negative pole grid after the vacuum drying is made into the foamed lead negative pole; (4) Winding: the positive...
PUM
Property | Measurement | Unit |
---|---|---|
Density | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com