Green cleaning energy-saving antiwear hydraulic oil and production process thereof
An anti-wear hydraulic oil and clean technology, applied in the field of lubricating oil, can solve problems such as easy pollution of lakes, rivers, oceans and groundwater systems, pollution of molasses light industrial products, product quality hidden dangers, etc., to achieve good compatibility and anti-wear properties Good, good degradation performance effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] Put 30 kg of hydrogenated paraffin base KVG46# oil refined by hydroisomerization, and 10 kg of synthetic hydrocarbon (polyα-olefin) PAO10 components into the blending kettle, stir and heat to 70°C, and then continue to put in refined camellia oil 20 kg, 20 kg of cottonseed oil, 96 kg of PAO2, 0.05 kg of phenolic antioxidant, fully stirred, after 2 hours, test its basic physical and chemical indicators, and then adjust the base oil according to the test results, and then put in the compounded B A total of 1 kg of propylene copolymer OCP 0080, 0030 and 0.5 kg of compounded antioxidant dialkyl dithiophosphate, 6 kg of compound vulcanized rapeseed oil and vulcanized animal oil, (wind-blown tea seed oil, lauryl alcohol, Stearic acid), 2.05 kilograms of metal activator, pour point depressant, antifoam agent fully mix to obtain product.
Embodiment 2
[0040] Add 35 kg of paraffin-based KVG46# oil refined by hydroisomerization and 18 kg of synthetic hydrocarbon (polyα-olefin) PAO10 components into the blending kettle, stir and heat to 70°C, and then continue to put in 30 kg of refined peanut oil , PAO2 9.5kg and phenolic antioxidant 0.1kg, fully stirred, after 2 hours, test its basic physical and chemical indicators, then adjust the base oil according to the test results, and then put in the compounded ethylene-propylene copolymer OCP 0080 0030, a total of 0.5 Kg and 0.5 kg of composite antioxidant dialkyl dithiophosphate, 1.5 kg of compound vulcanized animal and vegetable oil, and 0.05 kg of metal deactivator, pour point depressant, and antifoaming agent are fully mixed to obtain the product.
Embodiment 3
[0042] Add 25 kg of hydroisomerized refined paraffinic base KVG46# oil, and 18 kg of synthetic hydrocarbon (polyα-olefin) PAO10 components into the blending kettle, stir and heat to 70°C, and then continue to put in refined tea seed oil for 38 kg, and 0.1 kg of phenolic antioxidant, POA6.10 kg, fully stirred, after 3 hours, test its basic physical and chemical indicators, then adjust the base oil according to the test results, and then put in the compounded ethylene-propylene copolymer OCP 0080, 0050 0.5 kg in total and 1 kg of compound antioxidant dialkyl dithiocarbamate, 2 kg of compound vulcanized animal and vegetable oil, 1.5 kg of methyl ester, 3.45 kg of polyoxymethylene acrylate and trimethyl propane grease, 0.05 kg of metal deactivator, antifoaming agent and pour point depressant are fully mixed to obtain the product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com