Heating composition and application thereof in food heating
A technology of exothermic composition and exothermic body, which is applied in the direction of heat exchange materials, heating devices, chemical instruments and methods, etc., can solve the problems of excessive exothermic rate, poor exothermic control, and non-environmental components, and achieve sustainable Long time, low cost, effect of increasing appetite
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0050] Under normal temperature conditions, 40 grams of epoxy soybean oil (epoxy value ≈ 6.3%), 22 grams of epoxy resin E-55 (epoxy value ≈ 0.56), 10 grams of vermiculite, 2.5 grams of A1 type ethyl maltol and Mix 0.5 grams of mint flavor evenly into a larger aluminum bag a, mix 15 grams of soybean oil, 2 grams of polyamide (number average molecular weight 200) and 8 grams of polysebacic anhydride into another smaller bag Seal in the aluminum bag b, then seal the smaller aluminum bag in the larger aluminum bag to obtain the epoxy soybean type self-heating food heating bag.
Embodiment 2
[0052]Under normal temperature conditions, 30 grams of epoxy soybean oil (epoxy value ≈ 6.3%), 20.42 grams of epoxy resin E-51 (epoxy value ≈ 0.50), 5 grams of vermiculite, 0.08 gram of A1 type ethyl maltol and Mix 2.50 grams of mint flavor evenly and put it into a larger aluminum bag a, mix 10 grams of soybean oil, 30 grams of polyamide (number average molecular weight of 200) and 2 grams of polysebacic anhydride and put it into another smaller bag Seal in the aluminum bag b, then seal the smaller aluminum bag in the larger aluminum bag to obtain the epoxy soybean type self-heating food heating bag.
Embodiment 3
[0054] Under normal temperature conditions, 4 grams of epoxy soybean oil (epoxy value ≈ 6.3%), 30 grams of epoxy resin E-31 (epoxy value ≈ 0.30), 10 grams of vermiculite, 2.5 grams of A1 type ethyl maltol and Mix 0.5 grams of mint flavor evenly and put it into a larger aluminum bag a, mix 15 grams of soybean oil, 30 grams of polyamide (number average molecular weight of 200) and 8 grams of polysebacic anhydride and put it into another smaller bag The aluminum bag b is sealed, and then the smaller aluminum bag is sealed in the larger aluminum bag I to obtain the epoxy soybean type self-heating food heating bag.
PUM
Property | Measurement | Unit |
---|---|---|
epoxy value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com