A petroleum sulfonate and modification technology, which is applied in the fields of sulfonate preparation, sulfonic acid preparation, chemical instruments and methods, etc., can solve problems such as inability to use in large quantities, achieve less usage, improve hard water resistance, and high catalytic activity Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Embodiment 1: Preparation of modified petroleum sulfonate
[0030] Including the following preparation steps:
[0031] Step 1: Add 400 g of high-aromatic raw material oil, 6 g of anhydrous p-toluenesulfonic acid, and 15 g of maleic anhydride into the reactor. The reaction kettle is sealed, 2-4g of anhydrous HCl gas is introduced through the air inlet, and the air inlet valve is closed. Set the reaction temperature to 60-70°C, start stirring, and react for 6-7h. Synthetic modified raw oil.
[0032] Step 2, add 100g modified raw material oil in the there-necked flask, add 300g dichloroethane to dissolve; Liquid 24g SO 3 Dissolve with 96g of dichloroethane, make sulfonating agent with a concentration of 20%, transfer the sulfonating agent to the dropping funnel; put the three-necked flask into a constant temperature water bath, set the reaction temperature to 20°C, start electric stirring, and stir The speed is 300-350rpm; put the dropping funnel with sulfonating agent...
Embodiment 2
[0037] Embodiment 2: Preparation of modified petroleum sulfonate
[0038] Including the following preparation steps:
[0039] Step 1: Add 400 g of wax oil, 4 g of anhydrous p-toluenesulfonic acid, and 12 g of acrylic acid into the reaction kettle. The reaction kettle was sealed, 3 g of anhydrous HCl gas was introduced through the air inlet, and the air inlet valve was closed. Set the reaction temperature to 60-70°C, start stirring, and react for 6-7h. Synthetic modified raw oil.
[0040] Step 2, add 150g modified raw material oil in the there-necked flask, add 150g dichloroethane to dissolve; Liquid 30g SO 3 Dissolve it with 120g of dichloroethane, configure it into a sulfonating agent with a concentration of 20%, transfer the sulfonating agent to the dropping funnel; put the three-neck flask into a constant temperature water bath, set the reaction temperature to 20°C, start the electric stirring, and stir The speed is 300-350rpm; put the dropping funnel with sulfonating a...
Embodiment 3
[0045] Embodiment 3: Preparation of modified petroleum sulfonate heavy oil viscosity reducer
[0046] Including the following preparation steps:
[0047]Step 1: Add 300 g of high-aromatic raw material oil, 6 g of anhydrous p-toluenesulfonic acid, 10 g of maleic anhydride, and 6 g of dodecene into the reactor. The reaction kettle was sealed, 4 g of anhydrous HCl gas was introduced through the gas inlet, and the gas inlet valve was closed. Set the reaction temperature to 60-70°C, start stirring, and react for 6-7h. Synthetic modified raw oil.
[0048] Step 2, add 100g modified raw material oil in the there-necked flask, add 300g dichloroethane to dissolve; Liquid 19g SO 3 Dissolve it with 76g of dichloroethane, configure it as a sulfonating agent with a concentration of 20%, transfer the sulfonating agent to the dropping funnel; put the three-necked flask into a constant temperature water bath, set the reaction temperature to 20°C, start the electric stirring, and stir The s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com