Antibacterial hydrophobic polymer as well as preparation method and application thereof
A polymer and hydrophobic technology, which is applied in the field of antibacterial materials, can solve the problems that antibacterial products cannot maintain antibacterial effect, washable service life, poor heat resistance, etc., and achieve long-lasting antibacterial effect of materials, long-lasting antibacterial effect, antibacterial The effect of excellent performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example 1
[0049]Guanidine-based polymers, including polyhexamethyleneguanidine hydrochloride, the preparation method of polyhexamethyleneguanidine hydrochloride is as follows:
[0050] Feed 93g of hexamethylenediamine and guanidine hydrochloride at a molar ratio of 0.8:1.1, then raise the temperature to 170°C, and react for 6 hours to obtain polyhexamethyleneguanidine hydrochloride.
preparation example 2
[0052] Guanidine-based polymers, including polyhexamethylene biguanide hydrochloride, the preparation method of polyhexamethylene biguanide hydrochloride is as follows:
[0053] A1. Add hydrochloric acid dropwise to 100 g of hexamethylenediamine, control the pH value of the solution to 5, continue the reaction for 1 hour after the addition, filter and dry to make hexamethylenediamine hydrochloride;
[0054] A2. Polyhexamethylenediamine hydrochloride and 100 g of sodium dicyandiamide in a molar ratio of 1.1:1 were polymerized at 145° C. for a reaction time of 11 hours to obtain polyhexamethylene biguanide hydrochloride.
Embodiment 1
[0057] A kind of antibacterial hydrophobic polymer, adopts following preparation method,
[0058] S1, 5g of guanidine-based polymer was dissolved in 25g of water, the mass ratio of guanidine-based polymer to water was 1:5, stirred until the guanidine-based polymer was completely dissolved to obtain a guanidinium salt solution;
[0059] S2, the guanidinium salt solution is placed in a water bath at 35°C, and 27.5g of a compound with a hydrophobic group is added in the guanidine salt solution, and the mass ratio between the guanidine salt solution and the compound with a hydrophobic group is 1: 1.1, stir for 5 hours, filter and dry to obtain the antibacterial hydrophobic polymer;
[0060] Wherein, the compound with a hydrophobic group in this embodiment is benzenesulfonic acid, and the guanidine-based polymer prepared in Preparation Example 1 is added to S1.
[0061] The synthetic structural formula of the antibacterial hydrophobic polymer of embodiment 1-5 is as follows:
[0...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com