Production method of safe and anti-deformation sliding window
A production method and technology of sliding windows, applied in the direction of the wing frame, etc., can solve the problems of easy aging deformation and low safety of sliding windows, and achieve the effects of improving the factory yield, increasing the bonding strength, and excellent aging resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] Embodiment 1: A production method of a safe anti-deformation sliding window, comprising the following steps:
[0026] 1) Pretreatment of raw materials: After pretreatment, the aluminum profiles used to make the sliding window frame are sent to the spraying room for plasma spraying treatment, in which nitrogen and oxygen are used as working gases to make the modified aluminum powder in the ionized gas Spray and deposit on the surface of the aluminum profile under the action of the load, and then place the sprayed aluminum profile in a curing furnace to bake for 20 to 30 minutes to obtain a corrosion-resistant aluminum profile;
[0027] 2) Calibration of processing equipment: First, use measuring tools to perform error correction processing on cutting and punching equipment. After the correction is completed, then conduct a pre-production to check whether the processing size is within the preset size range of the drawing. If the error of the processing size exceeds the dra...
Embodiment 2
[0034] Embodiment 2: A production method of a safe anti-deformation sliding window, comprising the following steps:
[0035] 1) Pretreatment of raw materials: After pretreatment, the aluminum profiles used to make the sliding window frame are sent to the spraying room for plasma spraying treatment, in which nitrogen and oxygen are used as working gases to make the modified aluminum powder in the ionized gas Spray and deposit on the surface of the aluminum profile under the action of the carrier, then place the sprayed aluminum profile in a curing furnace and bake for 20 to 30 minutes to obtain a corrosion-resistant aluminum profile. Add antioxidants, ultraviolet absorbers and anti Mildew and antibacterial agent, anti-aging sealing strip;
[0036] 2) Calibration of processing equipment: First, use measuring tools to perform error correction processing on cutting and punching equipment. After the correction is completed, then conduct a pre-production to check whether the process...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com