Surface treatment process of furniture
A technology for surface treatment and furniture. It is used in devices and coatings that apply liquid to the surface. It can solve problems such as dry cracking and mildew, and achieve the effects of extending service life, good water resistance and high connection strength.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A surface treatment process for furniture, said treatment process comprising the following steps:
[0023] (1) Polishing: Clean the surface of the furniture to be treated first, dry it, and then polish it with sandpaper.
[0024] (2) Criticize the dust: scrape the putty layer on the surface of the furniture, the thickness of the putty layer is 0.8mm; coat the putty layer 3-4 times, the putty layer is scraped with a horn board, and the mass composition of the putty layer is : 10 parts of raw lacquer, 2 parts of paris plaster powder, 2 parts of silicon dioxide, 10 parts of water.
[0025] (3) Coloring: After the putty layer in step (2) is completely dry, sand it with sandpaper, and then paint with azo pigments; the drying temperature of the putty layer is 20-24°C.
[0026] (4) Roller coating primer and raw lacquer: After sanding with sandpaper after coloring, spray the primer in the paint room. After the primer is completely dry, roll the raw lacquer layer, and roll the ...
Embodiment 2
[0028] A surface treatment process for furniture, said treatment process comprising the following steps:
[0029] (1) Polishing: Clean the surface of the furniture to be treated first, dry it, and then polish it with sandpaper.
[0030] (2) Criticize the dust: scrape the putty layer on the surface of the furniture, the thickness of the putty layer is 0.9mm; coat the putty layer 3-4 times, the putty layer is scraped with a horn board, and the mass composition of the putty layer is : Raw lacquer 13 parts, Paris plaster powder 4 parts, silicon dioxide 3.5 parts, water 13 parts.
[0031] (3) Coloring: After the putty layer in step (2) is completely dry, sand it with sandpaper, and then paint it with lake pigments; the drying temperature of the putty layer is 20-24°C.
[0032] (4) Roller coating primer and raw lacquer: After sanding with sandpaper after coloring, spray the primer in the paint room. After the primer is completely dry, roll the raw lacquer layer, and roll the paint ...
Embodiment 3
[0034] A surface treatment process for furniture, said treatment process comprising the following steps:
[0035] (1) Polishing: Clean the surface of the furniture to be treated first, dry it, and then polish it with sandpaper.
[0036] (2) Criticize the dust: scrape the putty layer on the surface of the furniture, the thickness of the putty layer is 1mm; coat the putty layer 3-4 times, and scrape the putty layer with a horn board. The mass components of the putty layer are as follows: 15 parts of raw lacquer, 5 parts of paris plaster powder, 4 parts of silicon dioxide, and 15 parts of water.
[0037] (3) Coloring: After the putty layer in step (2) is completely dry, sand it with sandpaper, and then color it. When coloring, use azo pigments, lake pigments, heterocyclic pigments, and polycyclic ketones One of pigments and phthalocyanine pigments; the drying temperature of the putty layer is 20-24 ° C,
[0038] (4) Roller coating primer and raw lacquer: After sanding with sand...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com