Beta-cyclodextrin/magnetic nanoparticle/Go electrochemical sensor
A technology of magnetic nanoparticles and cyclodextrin, applied in the direction of material electrochemical variables, scientific instruments, nanotechnology, etc., can solve the problem of high manufacturing cost, and achieve the effect of fast electron transfer, strong catalytic ability, and good dispersion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] A kind of β-cyclodextrin / magnetic nanoparticles (Fe 3 o 4 -MnO 2 ) / graphene oxide (GO) electrochemical sensor, its manufacture method comprises the steps:
[0036] 1) Preparation of magnetic nanoparticles / GO composites
[0037] Add FeSO to 30 mL of graphene oxide solution with a concentration of 0.3 mg / mL 4 ·7H 2 O 0.3g, stirred to dissolve, heated in a water bath to 80°C, added 5mL of 2mol / L NaOH solution under the protection of an inert atmosphere, a yellow-green precipitate appeared in the solution, and the concentration was 0.1mol / L KMnO 4 Add 0.8mL of the solution to the above solution, the solution turns from yellow-green to brown, keep warm for 3 hours, centrifuge and wash until neutral, and vacuum dry at 50°C for later use;
[0038] 2) Preparation of β-cyclodextrin / magnetic nanoparticles / GO composites
[0039] Weigh 0.1 g of the magnetic nanoparticle / graphene oxide composite material obtained in step (1) into 40 mL of water, add 0.1 g of β-cyclodextrin, re...
Embodiment 2
[0043] A kind of β-cyclodextrin / magnetic nanoparticles / GO composite material, its preparation method is:
[0044] 1) Preparation of magnetic nanoparticles / GO composites
[0045]Take 20 mL of graphene oxide solution with a concentration of 0.2 mg / mL, add 0.2 g of ferrous sulfate heptahydrate, stir to fully dissolve ferrous sulfate heptahydrate, heat in a water bath to 70 °C, and add 2 mol / L hydrogen under the protection of an inert atmosphere Sodium oxide 2mL, when the yellow-green precipitate appears, add 0.4mL of potassium permanganate solution to it, wait for the yellow-green precipitate to turn into a brown solution, keep warm for 2h, centrifuge and wash until neutral, and dry in vacuum at 50°C;
[0046] 2) Preparation of β-cyclodextrin / magnetic nanoparticles / GO composites
[0047] Weigh 0.1 g of the magnetic nanoparticle / GO composite material obtained in step (1) into 40 mL of water, add 0.1 g of β-cyclodextrin, react in a constant temperature water bath at 58 °C for 4 h,...
Embodiment 3
[0049] A kind of β-cyclodextrin / magnetic nanoparticles / GO composite material, its preparation method is:
[0050] 1) Preparation of magnetic nanoparticles / GO composites
[0051] Take 50 mL of graphene oxide solution with a concentration of 0.5 mg / mL, add 1.0 g of ferrous sulfate heptahydrate, stir to fully dissolve ferrous sulfate heptahydrate, heat in a water bath to 90°C, and add 2 mol / L hydrogen under the protection of an inert atmosphere Sodium oxide 10mL, when the yellow-green precipitate appears, add 0.8mL of potassium permanganate solution to it, wait for the yellow-green precipitate to turn into a brown solution, keep it warm for 4 hours, centrifuge and wash until neutral, and dry it under vacuum at 50°C;
[0052] 2) Preparation of β-cyclodextrin / magnetic nanoparticles / GO composites
[0053] Weigh 0.2 g of the magnetic nanoparticle / GO composite material obtained in step (1) into 40 mL of water, add 0.2 g of β-cyclodextrin, react in a constant temperature water bath at...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com