Fluorite ore flotation collecting agent
A technology of collectors and fluorite ore, which is applied in the field of mineral flotation collectors and flotation collectors, can solve the problems of low selectivity, poor antifreeze ability, poor dispersibility, etc., and achieves the preparation method Simple, low cost, and the effect of improving the concentrate grade
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The fluorite ore flotation collector of the present embodiment is prepared from the following raw materials in weight percentage: phenylaminophosphoric acid 50%, oleic acid 30%, sodium alkylsulfonate 15%, water glass 5%, according to the above Weigh the raw materials in percentage by weight, heat oleic acid to 60°C-70°C, add phenylaminophosphoric acid and stir, then add sodium alkylsulfonate and stir, finally add water glass and stir for 1 hour, and stir evenly to obtain Fluorite ore flotation collector.
[0024] Using the prepared fluorite ore flotation collector, the flotation grade is 42.73% of the raw ore, the obtained titanium concentrate grade is 92.56%, and the recovery rate is a good indicator of 87.23%.
Embodiment 2
[0026] The fluorite ore flotation collector of the present embodiment is prepared from the following raw materials in weight percentage: phenylaminophosphoric acid 51%, oleic acid 29%, sodium alkylsulfonate 15%, water glass 5%, according to the above Weigh the raw materials in percentage by weight, heat oleic acid to 60°C-70°C, add phenylaminophosphoric acid and stir, then add sodium alkylsulfonate and stir, finally add water glass and stir for 1 hour, and stir evenly to obtain Fluorite ore flotation collector.
[0027] Using the prepared fluorite ore flotation collector, the flotation grade is 42.73% of the raw ore, the obtained titanium concentrate grade is 92.17%, and the recovery rate is a good indicator of 87.02%.
Embodiment 3
[0029] The fluorite ore flotation collector of the present embodiment is prepared from the following raw materials in weight percentage: phenylaminophosphoric acid 52%, oleic acid 28%, sodium alkylsulfonate 15%, water glass 5%, according to the above Weigh the raw materials in percentage by weight, heat oleic acid to 60°C-70°C, add phenylaminophosphoric acid and stir, then add sodium alkylsulfonate and stir, finally add water glass and stir for 1 hour, and stir evenly to obtain Fluorite ore flotation collector.
[0030] Using the prepared fluorite ore flotation collector, the flotation grade is 42.73% of the raw ore, the obtained titanium concentrate grade is 92.09%, and the recovery rate is a good indicator of 86.57%.
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com