High-temperature-resistant oil slurry scale inhibitor
A technology of antiscalant and high temperature resistance, which is applied in the petroleum industry, treatment of hydrocarbon oil, treatment of equipment corrosion/inhibition of fouling, etc. It can solve the problems of affecting the life of catalytic cracking catalysts, the use effect is not obvious, and the price of antiscalants is expensive. Achieve the effects of inhibiting coking and scaling, inhibiting condensation and dehydrogenation reactions, and good dispersion effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] A high-temperature oil slurry scale inhibitor, comprising the following components in mass fraction: polyisobutylene maleic anhydride (detergent and dispersant) 7%, bis-succinimide (detergent and dispersant) 13%, 4,4-di Isooctyl diphenylamine (amine type antioxidant) 0.1%, decahydronaphthalene (hydrogen donating type antioxidant) 5%, tolyltriazole (metal deactivator) 2%, the balance is S150 aromatic hydrocarbon oil solvent . Its preparation method is as follows: first, heat the solvent to 40-60°C, then add the remaining components in proportion, and stir at 40-60°C for 30 minutes to obtain the high-temperature oil slurry scale inhibitor.
Embodiment 2
[0026] A high-temperature oil slurry scale inhibitor, comprising the following components in mass fraction: polyisobutylene maleic anhydride (detergent and dispersant) 15%, bis-succinimide (detergent and dispersant) 15%, didodecyl Diphenylamine (amine type antioxidant) 2%, tetralin (hydrogen donating type antioxidant) 2%, tolyltriazole (metal deactivator) 1%, the balance is diesel oil. The preparation method is as follows: first, heat the solvent to 40-60°C, then add the remaining components in proportion, and stir at 40-60°C for 35 minutes to obtain the high-temperature oil slurry scale inhibitor.
Embodiment 3
[0028] A high-temperature oil slurry scale inhibitor, comprising the following components in mass fractions: polyisobutylene maleic anhydride (detergent and dispersant) 20%, monosuccinimide (detergent and dispersant) 15%, styryl octyl Diphenylamine (amine type antioxidant) 5%, benzyl alcohol (hydrogen donating type antioxidant) 0.1%, thiadiazole (metal deactivator) 0.1%, and the balance is S150 aromatic hydrocarbon oil solvent. The preparation method is as follows: first, heat the solvent to 40-60°C, then add the remaining components in proportion, and stir at 40-60°C for 25 minutes to obtain the high-temperature oil slurry scale inhibitor.
PUM
Property | Measurement | Unit |
---|---|---|
dew point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com