A technology of biomass and phosphorus-locking agent, which is applied in the direction of biological sludge treatment, water pollutants, sludge treatment, etc., can solve the problem of removing phosphorus from water body sediment, and achieve the effect of efficient in-situ removal of phosphorus from sediment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A biomass phosphorus-locking agent comprises: dewatered sludge, rice husk powder, organic meal waste, clinker and shell powder. Its preparation method comprises the following steps:
[0024] (1) Preparation of fermented sludge: dehydrated sludge, clinker, organic meal waste and rice husk powder were mixed according to the mass ratio of 1:1:1:1.5 and naturally fermented for 1.5 months, and stirred and mixed every 12 hours for 1 times, get fermented sludge;
[0025] (2) Preparation of biomass phosphorus-locking agent: fermented sludge and shell powder are mixed at a mass ratio of 2:1, placed in a sealed tank for carbonization, and the temperature is raised from room temperature to 400 °C at a heating rate of 3 °C / min. Then pyrolyze at 400°C for 34 hours, and then cool to room temperature to obtain a biomass phosphorus-locking agent.
[0026] A method for in-situ removal of phosphorus from polluted water body sediment by using a biomass phosphorus-locking agent, specific...
Embodiment 2
[0028] A biomass phosphorus-locking agent comprises: dewatered sludge, corn stalk powder, organic meal waste, clinker and shell powder. Its preparation method comprises the following steps:
[0029] (1) Preparation of fermented sludge: dehydrated sludge, clinker, organic meal waste and corn stalk powder were mixed according to the mass ratio of 1:1:1:2 and naturally fermented for 2 months, and stirred and mixed every 14 hours for 1 times, get fermented sludge;
[0030] (2) Preparation of biomass phosphorus-locking agent: fermented sludge and shell powder are mixed in a mass ratio of 3:1 and then placed in a sealed tank for carbonization. The temperature is raised from room temperature to 420 °C at a heating rate of 5 °C / min. Then pyrolyze at 420° C. for 3 hours, and then cool to room temperature to obtain a biomass phosphorus-locking agent.
[0031] A method for in-situ removal of phosphorus from polluted water body sediment by using a biomass phosphorus-locking agent, speci...
Embodiment 3
[0033] A biomass phosphorus-locking agent comprises: dewatered sludge, sawdust powder, organic meal waste, clinker and shell powder. Its preparation method comprises the following steps:
[0034](1) Preparation of fermented sludge: dehydrated sludge, clinker, organic meal waste and sawdust powder are mixed in a mass ratio of 1:1:1:1 and naturally fermented for 1 month, and stirred once every 12 hours , get fermented sludge;
[0035] (2) Preparation of biomass phosphorus-locking agent: fermented sludge and shell powder are mixed at a mass ratio of 1:1, placed in a sealed tank for carbonization, and the temperature is raised from room temperature to 380°C at a heating rate of 2°C / min. Then pyrolyze at 380° C. for 5 hours, and then cool to room temperature to obtain a biomass phosphorus-locking agent.
[0036] A method for in-situ removal of phosphorus from sediments in polluted water bodies by utilizing a biomass phosphorus-locking agent, specifically: mixing the biomass phosp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com