Biomass phosphorus-locking agent and method for in-situ removal of phosphorus from polluted water body sediment
A technology of biomass and phosphorus-locking agent, applied in biological sludge treatment, sludge treatment, water pollutants, etc., can solve the problem of removing phosphorus in water body sediment, and achieve the effect of high-efficiency in-situ removal of phosphorus in sediment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A biomass phosphorus-locking agent comprises: dewatered sludge, rice husk powder, organic meal waste, clinker and shell powder. Its preparation method comprises the following steps:
[0024] (1) Preparation of fermented sludge: dehydrated sludge, clinker, organic meal waste and rice husk powder were mixed according to the mass ratio of 1:1:1:1.5 and naturally fermented for 1.5 months, and stirred and mixed every 12 hours for 1 times, get fermented sludge;
[0025] (2) Preparation of biomass phosphorus-locking agent: fermented sludge and shell powder are mixed at a mass ratio of 2:1, placed in a sealed tank for carbonization, and the temperature is raised from room temperature to 400 °C at a heating rate of 3 °C / min. Then pyrolyze at 400°C for 34 hours, and then cool to room temperature to obtain a biomass phosphorus-locking agent.
[0026] A method for in-situ removal of phosphorus from polluted water body sediment by using a biomass phosphorus-locking agent, specific...
Embodiment 2
[0028] A biomass phosphorus-locking agent comprises: dewatered sludge, corn stalk powder, organic meal waste, clinker and shell powder. Its preparation method comprises the following steps:
[0029] (1) Preparation of fermented sludge: dehydrated sludge, clinker, organic meal waste and corn stalk powder were mixed according to the mass ratio of 1:1:1:2 and naturally fermented for 2 months, and stirred and mixed every 14 hours for 1 times, get fermented sludge;
[0030] (2) Preparation of biomass phosphorus-locking agent: fermented sludge and shell powder are mixed in a mass ratio of 3:1 and then placed in a sealed tank for carbonization. The temperature is raised from room temperature to 420 °C at a heating rate of 5 °C / min. Then pyrolyze at 420° C. for 3 hours, and then cool to room temperature to obtain a biomass phosphorus-locking agent.
[0031] A method for in-situ removal of phosphorus from polluted water body sediment by using a biomass phosphorus-locking agent, speci...
Embodiment 3
[0033] A biomass phosphorus-locking agent comprises: dewatered sludge, sawdust powder, organic meal waste, clinker and shell powder. Its preparation method comprises the following steps:
[0034](1) Preparation of fermented sludge: dehydrated sludge, clinker, organic meal waste and sawdust powder are mixed in a mass ratio of 1:1:1:1 and naturally fermented for 1 month, and stirred once every 12 hours , get fermented sludge;
[0035] (2) Preparation of biomass phosphorus-locking agent: fermented sludge and shell powder are mixed at a mass ratio of 1:1, placed in a sealed tank for carbonization, and the temperature is raised from room temperature to 380°C at a heating rate of 2°C / min. Then pyrolyze at 380° C. for 5 hours, and then cool to room temperature to obtain a biomass phosphorus-locking agent.
[0036] A method for in-situ removal of phosphorus from sediments in polluted water bodies by utilizing a biomass phosphorus-locking agent, specifically: mixing the biomass phosp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com