[0027] A method of painting on leather, comprising the following steps,
[0028] Step 1, engrave the texture, select the whole piece of leather, and use a carving knife to carve the basic work on the whole piece of leather;
[0029] Step 2, punching, after the basic carving of the work is completed, use the pinholes to perforate and soak the entire leather along the carving lines of the work;
[0030] Step 3: Soak in water, select the whole piece of leather in warm water at 50-55°C, soak for 1-1.2 hours until the water absorption state reaches 40-50%, then filter it, and use a rolling roller to flatten the whole piece of leather ;
[0031] Step 4, brushing, adding 5-8g of cleaning solvent, 6-8g of moisturizing agent, and brushing and cleaning the entire leather surface with a brush;
[0032] Step 5: Fatliquoring and softening. Mix the fatliquoring agent and white vinegar according to the weight ratio of 1:6. After mixing, add warm water at 65-70°C. Use a scrub brush to evenl...
Embodiment 2
[0040] A method of painting on leather, comprising the following steps,
[0041] Step 1, engrave the texture, select the whole piece of leather, and use a carving knife to carve the basic work on the whole piece of leather;
[0042] Step 2, punching, after the basic carving of the work is completed, use the pinholes to perforate and soak the entire leather along the carving lines of the work;
[0043] Step 3: Soak in water, select the whole piece of leather in warm water at 50-55°C, soak for 1-1.2 hours until the water absorption state reaches 40-50%, then filter it, and use a rolling roller to flatten the whole piece of leather ;
[0044] Step 4, brushing, adding 5-8g of cleaning solvent, 6-8g of moisturizing agent, and brushing and cleaning the entire leather surface with a brush;
[0045] Step 5: Fatliquoring and softening. Mix the fatliquoring agent and white vinegar according to the weight ratio of 1:6. After mixing, add warm water at 65-70°C. Use a scrub brush to evenl...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com