preparation example Construction
[0024] The preparation of several soluble rare earth nitrates is just an example and not limited.
[0025] Tb(NO 3 ) 3 ·6H 2 The preparation of O comprises the steps of: according to the molar ratio of terbium element in terbium oxide and nitrogen element in concentrated nitric acid is the ratio of 1:8, weigh Tb 2 o 3 In a beaker, add concentrated nitric acid to dissolve it completely, stop after heating and stirring to evaporate excess water and nitric acid, and wait for it to cool and crystallize to obtain Tb(NO 3 ) 3 ·6H 2 O.
[0026] Eu(NO 3 ) 3 ·6H 2 The preparation of O comprises the steps of: weighing Eu 2 o 3 In a beaker, add concentrated nitric acid to dissolve it completely, stop after heating and stirring to evaporate excess water and nitric acid, wait for it to cool and crystallize to obtain Eu(NO 3 ) 3 ·6H 2 O.
[0027] Dy(NO 3 ) 3 ·6H 2 The preparation of O comprises the steps of: taking Dy 2 o 3 In a beaker, add concentrated nitric acid to di...
Embodiment 1
[0031] The preparation method of rare earth nucleoside fluorescent hydrogel comprises the following steps:
[0032] (1) with Tb(NO 3 ) 3 ·6H 2 O prepares Tb(NO with a mass concentration of 2%) 3 ) 3 Aqueous solution, preparing a deoxythymidine aqueous solution with a mass concentration of 2%;
[0033] (2) Tb(NO 3 ) 3 Mix the aqueous solution and the deoxythymidine aqueous solution at a volume ratio of 1:1, adjust the pH value to 8 with dilute ammonia water, raise the temperature to 65°C, let the reaction stand for 15 minutes, cool down to room temperature, and let it stand for 2 hours to obtain rare earth nucleoside fluorescent water gel. See figure 1 and figure 2 .
[0034] Depend on figure 1 It can be seen that the rare earth nucleoside fluorescent hydrogel obtained in this example is transparent and clear under fluorescent light.
[0035] Depend on figure 2 It can be seen that the rare earth nucleoside fluorescent hydrogel obtained in this example emits green...
Embodiment 2
[0037] The preparation method of rare earth nucleoside fluorescent hydrogel comprises the following steps:
[0038] (1) with Eu(NO 3 ) 3 ·6H 2 O prepared Eu(NO with a mass concentration of 3% 3 ) 3 Aqueous solution, preparing a deoxythymidine aqueous solution with a mass concentration of 3%;
[0039] (2) Eu(NO 3 ) 3 The aqueous solution and the deoxythymidine aqueous solution are mixed uniformly at a ratio of 1:1 by volume, and the pH value is adjusted to 7 with dilute ammonia water, heated to 55°C, left to react for 20 minutes, cooled to room temperature, and left to stand for 4 hours to obtain rare earth nucleoside fluorescent water gel. See image 3 and Figure 4 .
[0040] Depend on image 3 It can be seen that the rare earth nucleoside fluorescent hydrogel obtained in this example is transparent and clear under fluorescent light.
[0041] Depend on Figure 4 It can be seen that the rare earth nucleoside fluorescent hydrogel obtained in this example emits red ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com