Embodiment 1
[0031] Embodiment 1, the preparation of porous hydroxyapatite
[0032] i) Take Tween-80 and add 100ml of toluene with a concentration of 0.5%. After shaking well, add 50ml of 1mol / L sodium carbonate solution, ultrasonic emulsification for 15min, and pour the emulsion into 300ml of 0.2mol / L calcium chloride solution. Stir and react for 2 hours, age for 24 hours, filter the aged solution with suction to obtain a white precipitate, wash with distilled water and absolute ethanol for 3 times, dry at 80°C for 12 hours, and obtain porous spherical calcium carbonate powder;
[0033] ii) Take the above-mentioned porous spherical calcium carbonate powder and add purified water to form a suspension of 0.05 g / ml. Under stirring conditions, add 0.03 mol / L disodium hydrogen phosphate solution to keep the pH at 11, stir for 12 hours, and age for 24 hours; filter the aged solution with suction to obtain a white precipitate, wash with distilled water and absolute ethanol three times, dry at 8...
Embodiment 2
[0034] Embodiment 2, preparation of anode furnace refining slag
[0035] S1. Sintering: take the copper-containing sludge and carry out sintering, move the sintered block into the smelting furnace, add limestone 10kg / t Cu, carbon fine 3kg / t Cu, and continuously feed in air containing 25% (v / v) oxygen at the same time Calcining to obtain blister copper, wherein the calcination temperature is 1100°C;
[0036] S2. Refining: move the above-mentioned blister copper into the refining furnace, add 3kg / t Cu heavy oil, and at the same time continue to feed air containing 95% (v / v) oxygen to mix the blister copper, add carbon powder 2kg / t Cu and 4kg / t Cu quartz stone to obtain anode copper plate and anode furnace refining slag, in which the calcining temperature is 1200°C.
[0037] The prepared anode furnace refining slag mainly includes the following components by weight: CaO 6.2-8.3wt%, SiO 2 25.6~29.2wt%, Al 2 o 3 6.3~9.4wt% and FeO 25.4~35.8wt%.
[0038] Table 1 The comp...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
crystallinity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com