A polyvinyl alcohol and drilling fluid technology, applied in the direction of drilling compositions, chemical instruments and methods, etc., can solve problems such as easy collapse and fracturing of the well wall, damage to temperature and pressure conditions, and reduction of fracture pressure, so as to avoid pore diameter Severe expansion, good low-temperature stability, and the effect of reducing repeated crushing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] Embodiment 1, the content of each component in the drilling fluid is: the mass ratio of polyvinyl alcohol is 1.8%, the mass ratio of sodium chloride is 4.5%, the mass ratio of potassium chloride is 4.5%, the mass ratio of ethylene glycol is 9%, the mass ratio of sulfur The mass ratio of phenolic resin SMP-2 is 1.8%, the mass ratio of potassium polyacrylate is 1.8%, the mass ratio of xanthan gum is 0.4%, the mass ratio of polyvinylpyrrolidone K90 is 0.8%, and the mass ratio of ethylene glycol ether is 0.8%, The mass ratio of mono-n-butyl glycol ether is 0.8%, and the rest is water for preparation.
Embodiment 2
[0035] Embodiment 2, the content of each component in the drilling fluid is: the mass ratio of polyvinyl alcohol is 2%, the mass ratio of sodium chloride is 5%, the mass ratio of potassium chloride is 5%, the mass ratio of ethylene glycol is 10%, the mass ratio of sulfur The mass ratio of phenolic resin SMP-2 is 2%, the mass ratio of potassium polyacrylate is 2%, the mass ratio of xanthan gum is 0.5%, the mass ratio of polyvinylpyrrolidone K90 is 1%, the mass ratio of ethylene glycol ether is 1%, The mass ratio of mono-n-butyl glycol ether is 1%, and the remaining components are preparation water.
Embodiment 3
[0036] Embodiment 3, the content of each component in the drilling fluid is: the mass ratio of polyvinyl alcohol is 2.2%, the mass ratio of sodium chloride is 5.5%, the mass ratio of potassium chloride is 5.5%, the mass ratio of ethylene glycol is 11%, the mass ratio of sulfur The mass ratio of phenolic resin SMP-2 is 2.2%, the mass ratio of potassium polyacrylate is 2.2%, the mass ratio of xanthan gum is 0.6%, the mass ratio of polyvinylpyrrolidone K90 is 1.2%, and the mass ratio of ethylene glycol ether is 1.2%, The mass ratio of mono-n-butyl glycol ether is 1.2%, and the rest is water for preparation.
[0037] The drilling fluid configuration methods of the above-mentioned examples 1, 2, and 3 are conventional drilling fluid configuration methods, and are evaluated by the following experimental methods:
[0038] 1 Evaluation of drilling fluid shale hydration inhibition
[0039] Inhibition evaluation experiment is an important part of the indoor evaluation of drilling fluid...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com