Embodiment 1
[0026] A degradable high-barrier composite material and a preparation method thereof, the composite material comprising the following steps:
[0027] (1) Preparation of the solution:
[0028] Tapioca starch solution: Dissolve 6.0 grams of tapioca starch in 100ml of distilled water, keep stirring in a water bath at 80°C for 30 minutes, and obtain a tapioca starch solution;
[0029] Polyvinyl alcohol solution: Dissolve 9.0 grams of polyvinyl alcohol in 100ml of distilled water, maintain it in a water bath at 95°C and stir for 30 minutes to obtain a polyvinyl alcohol solution;
[0030] Chitosan solution: Dissolve 3.0 grams of chitosan in 100 ml of 5% acetic acid solution, and ultrasonically disperse in an ultrasonic cleaner for 30 minutes to obtain a chitosan solution.
[0031] (2) Tapioca starch / polyvinyl alcohol / chitosan thin composite material preparation:
[0032] Add the above polyvinyl alcohol solution and chitosan solution into the tapioca starch solution, and add 10mL a...
Embodiment 2
[0034] A degradable high-barrier composite material and a preparation method thereof, the composite material comprising the following steps:
[0035] (1) Preparation of the solution:
[0036] Tapioca starch solution: Dissolve 6.0 grams of tapioca starch in 100ml of distilled water, keep stirring in a water bath at 80°C for 30 minutes, and obtain a tapioca starch solution;
[0037] Polyvinyl alcohol solution: Dissolve 9.0 grams of polyvinyl alcohol in 100ml of distilled water, maintain it in a water bath at 95°C and stir for 30 minutes to obtain a polyvinyl alcohol solution;
[0038] Chitosan solution: Dissolve 3.0 grams of chitosan in 100 ml of 5% acetic acid solution, and ultrasonically disperse in an ultrasonic cleaner for 30 minutes to obtain a chitosan solution.
[0039] (2) Tapioca starch / polyvinyl alcohol / chitosan thin composite material preparation:
[0040] Add the above polyvinyl alcohol solution and chitosan solution into the tapioca starch solution, and add 10mL a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com