Method for preparing novel energy-saving heat-insulating material
A thermal insulation material, a new type of technology, applied in the field of building materials, can solve the problems of high thermal conductivity, smoke toxicity, flammability, etc., and achieve good thermal insulation performance, good weather resistance, and good durability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A preparation method of a novel energy-saving thermal insulation material, comprising the following preparation steps:
[0026] a. Mix bentonite, slag, fly ash, quartz sand and saline solution, stir evenly at a high speed, the stirring speed is 600r / min, and stir for 40min to obtain slurry 1;
[0027] b. Mix fibers, polystyrene foam particles, water glass, redispersible latex powder, foaming agent, foam stabilizer and water into the foaming device, heat and fill inert gas for foaming reaction, temperature At 70°C, react for 25 minutes to obtain slurry 2;
[0028] c. Slowly stir slurry 2 and filter after defoaming to remove solid particles to obtain slurry 3;
[0029] d. Mix slurry 1 and slurry 3, add calcium carbide, water reducer, titanium dioxide, chitosan and hollow glass microspheres, pressurize at high temperature and stir at high speed, the stirring speed is 1500r / min, stir for 15min, then Inject into a twin-screw extruder, melt and extrude, and then introduce i...
Embodiment 2
[0039] A preparation method of a novel energy-saving thermal insulation material, comprising the following preparation steps:
[0040] a. Mix bentonite, slag, fly ash, quartz sand and saline solution, stir evenly at a high speed, the stirring speed is 600r / min, and stir for 30min to obtain slurry 1;
[0041] b. Mix fibers, polystyrene foam particles, water glass, redispersible latex powder, foaming agent, foam stabilizer and water into the foaming device, heat and fill inert gas for foaming reaction, temperature At 75°C, react for 25 minutes to obtain slurry 2;
[0042] c. Slowly stir slurry 2 and filter after defoaming to remove solid particles to obtain slurry 3;
[0043] d. Mix slurry 1 and slurry 3, add calcium carbide, water reducer, titanium dioxide, chitosan and hollow glass microspheres, pressurize at high temperature and stir at high speed, the stirring speed is 1200r / min, stir for 10min, then Inject into a twin-screw extruder, melt and extrude, and then introduce i...
Embodiment 3
[0053] A preparation method of a novel energy-saving thermal insulation material, comprising the following preparation steps:
[0054] a. Mix bentonite, slag, fly ash, quartz sand and saline solution, stir evenly at a high speed, the stirring speed is 800r / min, and stir for 40min to obtain slurry 1;
[0055] b. Mix fibers, polystyrene foam particles, water glass, redispersible latex powder, foaming agent, foam stabilizer and water into the foaming device, heat and fill inert gas for foaming reaction, temperature At 85°C, react for 35 minutes to obtain slurry 2;
[0056] c. Slowly stir slurry 2 and filter after defoaming to remove solid particles to obtain slurry 3;
[0057] d. Mix slurry 1 and slurry 3, add calcium carbide, water reducer, titanium dioxide, chitosan and hollow glass microspheres, pressurize at high temperature and stir at high speed, the stirring speed is 1200r / min, stir for 15min, then Inject into a twin-screw extruder, melt and extrude, and then introduce i...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com