Glazing technology of Jun porcelain glaze material with health care effects
A technology of Jun porcelain and glaze, applied in the field of ceramics, can solve the problems of poor antibacterial effect, low stability such as heat resistance, decomposed products or volatile products that are harmful to the human body, etc., to achieve the effect of promoting cell metabolism and improving endocrine
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] A kind of glazing process of Jun porcelain glaze with health care function, comprising the following steps:
[0036] (1) According to parts by weight, take 30~50 parts of green long-lasting luminescent powder SrO·Al 2 o 3 0.05B 2 o 3 : Dy, Eu, albite 30~40 parts, quartz 50~60 parts, calcite 10~15 parts, calcined kaolin 15~20 parts, spodumene 12~15 parts, talcum powder 5~8 parts and tin oxide 2 ~3 parts, crush the above-mentioned various raw materials, put them into a ball mill, add water to carry out wet grinding for 5~6 hours, and obtain glaze slurry after sieving, and set aside;
[0037] (2) To prepare a titanium dioxide microsphere carrier with a particle size of 30-32nm, add titanium dioxide to the In the mixed aqueous solution of silver nitrate and cerium nitrate, stir at a speed of 200~300r / min under the condition of constant temperature water bath at 50~70℃, then carry out suction filtration and drying, put it into a sintering furnace and calcinate at 400~600...
Embodiment 2
[0043] A kind of glazing process of Jun porcelain glaze with health care function, comprising the following steps:
[0044] (1) According to parts by weight, take 30~50 parts of blue long-lasting luminescent powder 4SrO·7Al 2 o 3 0.07B 2 o 3 : Nd, Eu, albite 30~40 parts, quartz 50~60 parts, calcite 10~15 parts, calcined kaolin 15~20 parts, spodumene 12~15 parts, talcum powder 5~8 parts and tin oxide 2 ~3 parts, crush the above-mentioned various raw materials, put them into a ball mill, add water to carry out wet grinding for 5~6 hours, and obtain glaze slurry after sieving, and set aside;
[0045] (2) To prepare a titanium dioxide microsphere carrier with a particle size of 30-32nm, add titanium dioxide to the In the mixed aqueous solution of silver nitrate and cerium nitrate, stir at a speed of 200~300r / min under the condition of constant temperature water bath at 50~70℃, then carry out suction filtration and drying, put it into a sintering furnace and calcinate at 400~60...
Embodiment 3
[0051] A kind of glazing process of Jun porcelain glaze with health care function, comprising the following steps:
[0052] (1) According to parts by weight, take 10~20 parts of blue long-lasting luminous powder 4SrO·7Al 2 o 3 0.07B 2 o 3 : Nd, Eu, green long-lasting luminous powder SrO·Al 2 o 3 0.05B 2 o 3 : Dy, Eu, albite 30~40 parts, quartz 50~60 parts, calcite 10~15 parts, calcined kaolin 15~20 parts, spodumene 12~15 parts, talcum powder 5~8 parts and tin oxide 2 ~3 parts, crush the above-mentioned various raw materials, put them into a ball mill, add water to carry out wet grinding for 5~6 hours, and obtain glaze slurry after sieving, and set aside;
[0053] (2) To prepare a titanium dioxide microsphere carrier with a particle size of 30-32nm, add titanium dioxide to the In the mixed aqueous solution of silver nitrate and cerium nitrate, stir at a speed of 200~300r / min under the condition of constant temperature water bath at 50~70℃, then carry out suction filtrat...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com