Preparation and use methods of environment-friendly nano composite colorful liquid wallpaper paint
A nano-composite, liquid wallpaper technology, applied in the field of colorful wall art coatings, can solve the problems of not containing long-term antibacterial ingredients and anti-aging peeling, not having anti-virus and sterilization, anti-mildew bright flash, affecting the use effect, etc. Achieve the effect of improving the decorative effect, strong anti-pollution, and making up for wall cracks
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0045] A preparation method of nanocomposite colorful liquid wallpaper paint, characterized in that said preparation method comprises the following steps:
[0046] (1) Prepare the following substances in parts by weight:
[0047] 80-90 parts of water,
[0048] Lithopone 25~30 parts,
[0049] 8-10 parts of nano calcium carbonate,
[0050] Nano silver solution 0.02-0.04 parts,
[0051] Aluminum silicate 2-4 parts,
[0052] Sodium hexametaphosphate 0.3~0.8 parts,
[0053] Nanoscale silicon dioxide 0.02~0.1 parts,
[0054] 0.5 parts of hydroxyethyl cellulose,
[0055] Particle size is 1200 mesh talcum powder 16-18 parts,
[0056] PH modifier 0.05~0.15 parts,
[0057] Nanoscale titanium dioxide 20~35 parts,
[0058] 2-4 parts of ethylene glycol,
[0059] Silicone modified acrylic resin 5-7 parts,
[0060] 1-2 parts of glycerin,
[0061] 0.1~0.4 parts of ethyl acrylate;
[0062] (2) Add water into the mixing tank, start the mixer and stir at a speed of 1000-1500r / min; ...
Embodiment 2
[0071] A preparation method of nanocomposite colorful liquid wallpaper paint, said preparation method comprising the following steps:
[0072] (1) Prepare the following substances in parts by weight:
[0073] 80-90 parts of water,
[0074] Lithopone 25~30 parts,
[0075] 8-10 parts of nano calcium carbonate,
[0076] Nano silver solution 0.02-0.04 parts,
[0077] Aluminum silicate 2-4 parts,
[0078] Sodium hexametaphosphate 0.3~0.8 parts,
[0079] Silicon dioxide 0.02~0.1 part,
[0080] 0.5 parts of hydroxyethyl cellulose,
[0081] 16-18 parts of talcum powder,
[0082] PH modifier 0.05~0.15 parts,
[0083] 20~35 parts of titanium dioxide,
[0084] 2-4 parts of ethylene glycol,
[0085] Silicone modified acrylic resin 5-7 parts,
[0086] 1-2 parts of glycerin,
[0087] 0.1~0.4 parts of methacrylic acid copolymer;
[0088] (2) Add water into the mixing tank, start the mixer and stir at a speed of 1000-1500r / min;
[0089] (3) Add titanium dioxide and silicon dioxide...
Embodiment 3
[0098] After diluting 4% clear water of a nanocomposite colorful liquid wallpaper paint prepared in Example 1, it can be sprayed, rolled or brushed.
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com