[0034] Embodiment 1: a kind of repairing method of depth scratch, it comprises the following steps:
[0035] Step 1: Use alcohol to clean up the dirt in the scratches;
[0036] Step 2: Use 1500# sandpaper to polish the scratches. The sandpaper uses long strips of soft sandpaper, and the sanding area is 3 ± 0.1 cm;
[0037] Step 3: Use scissors to cut the cigarette paper into long strips of the same size as the scratches, and use the long strips of paper to fill the scratches with the paint prepared by paint and thinner at a weight ratio of 1:4, requiring fullness , fill 3 times, the thinner the better each time, and bake each time with an infrared oven; the temperature of the infrared oven is 75°C, and the time is 3 minutes;
[0038] Step 4: Use a fine brush to dip the prepared saliva and thinner according to the weight ratio of 1:5. Apply the saliva around the scratch, and then bake it with an infrared oven. The temperature of the infrared oven is 70 ° C, and the time is 5 ...
Embodiment 2
[0047] Embodiment 2: a kind of repairing method of depth scratch, it comprises the following steps:
[0048] Step 1: Use alcohol to clean up the dirt in the scratches;
[0049] Step 2: Use 1500# sandpaper to polish the scratches. The sandpaper uses long strips of soft sandpaper, and the sanding area is 3 ± 0.1 cm;
[0050] Step 3: Use scissors to cut the cigarette paper into long strips of the same size as the scratches, and use the long strips of paper to fill the scratches with the paint prepared by paint and thinner at a weight ratio of 1:4, requiring fullness , filling 4 times, the thinner the filling the better each time, each time should be baked with an infrared oven; the temperature of the infrared oven is 85°C, and the time is 5 minutes;
[0051] Step 4: Use a fine brush to dip the prepared saliva and thinner according to the weight ratio of 1:5. Apply the saliva around the scratch, and then bake it with an infrared oven. The temperature of the infrared oven is 85°C,...
Embodiment 3
[0060] Embodiment 3: a kind of repairing method of depth scratch, it comprises the following steps:
[0061] Step 1: Use alcohol to clean up the dirt in the scratches;
[0062] Step 2: Use 1500# sandpaper to polish the scratches. The sandpaper uses long strips of soft sandpaper, and the sanding area is 3 ± 0.1 cm;
[0063] Step 3: Use scissors to cut the cigarette paper into long strips of the same size as the scratches, and use the long strips of paper to fill the scratches with the paint prepared by paint and thinner at a weight ratio of 1:4, requiring fullness , fill 5 times, the thinner the better each time, and bake each time with an infrared oven; the temperature of the infrared oven is 80°C, and the time is 4 minutes;
[0064] Step 4: Use a fine brush to dip the prepared saliva and the thinner according to the weight ratio of 1:5 to apply the saliva around the scratch, and then bake it with an infrared baking lamp. The temperature of the infrared baking lamp is 75 ℃, a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com