High-strength composite fiber non-woven cloth and preparation method thereof
A composite fiber, weft-free technology, applied in chemical instruments and methods, protective equipment, other household appliances, etc., can solve the problem of life and property safety not being guaranteed, and achieve the protection of life and property safety and good insulation effect. , the effect of tight connection
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A high-strength composite fiber non-weft cloth and a preparation method thereof, comprising the following steps:
[0022] S1. Use ultra-high-strength high-modulus polyethylene fiber as the base material.
[0023] S2. After uniform laying of polyethylene fibers, a series of uniform, parallel and straight arrangements are performed.
[0024] S3, put in the modified epoxy resin solution in the environment of 60-80 degrees for gluing.
[0025] S4. Composite laminating the formed polyethylene fiber layer to form a non-weft cloth, and the polyethylene fiber layer can be made into a 6-layer, 8-layer or 12-layer composite non-weft cloth.
[0026] The modified epoxy resin solution is mixed with binders, fillers, insulating fillers, flame retardants, white carbon black and alcohol. The binder is one of animal glue, synthetic resin, rubber or paint. The curing agent is one or more of vinyl triamine, amine ethyl piperazine, m-phenylenediamine or diaminodiphenylmethane, the mass o...
Embodiment 2
[0028] A high-strength composite fiber non-weft cloth and a preparation method thereof, comprising the following steps:
[0029] S1. Use ultra-high-strength high-modulus polyethylene fiber as the base material.
[0030] S2. After uniform laying of polyethylene fibers, a series of uniform, parallel and straight arrangements are performed.
[0031] S3, put in the modified epoxy resin solution in the environment of 60-80 degrees for gluing.
[0032] S4. Composite laminating the formed polyethylene fiber layer to form a non-weft cloth, and the polyethylene fiber layer can be made into a 6-layer, 8-layer or 12-layer composite non-weft cloth.
[0033] The modified epoxy resin solution is mixed with binder, filler, insulating filler, white carbon black and alcohol. The binder is one of animal glue, synthetic resin, rubber or paint, and the curing agent is ethylene. One or more of triamine, aminoethylpiperazine, m-phenylenediamine or diaminodiphenylmethane, the quality of hydroxynit...
Embodiment 3
[0035] A high-strength composite fiber non-weft cloth and a preparation method thereof, comprising the following steps:
[0036] S1. Use ultra-high-strength high-modulus polyethylene fiber as the base material.
[0037] S2. After uniform laying of polyethylene fibers, a series of uniform, parallel and straight arrangements are performed.
[0038] S3, put in the modified epoxy resin solution in the environment of 60-80 degrees for gluing.
[0039] S4. Composite laminating the formed polyethylene fiber layer to form a non-weft cloth, and the polyethylene fiber layer can be made into a 6-layer, 8-layer or 12-layer composite non-weft cloth.
[0040] The modified epoxy resin solution is mixed with binder, filler, insulating filler, white carbon black and alcohol. The binder is one of animal glue, synthetic resin, rubber or paint, and the curing agent is ethylene. One or more of triamine, aminoethylpiperazine, m-phenylenediamine or diaminodiphenylmethane, the quality of hydroxybut...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com