Capri blue crystal bead rough and preparation method thereof

A crystal bead and color technology, applied in glass manufacturing equipment, manufacturing tools, glass molding, etc., can solve problems such as unsuitable for continuous mass production, unstable product quality, low production efficiency, etc., and achieve lead-free dust pollution , good gloss, no dust pollution effect

Inactive Publication Date: 2017-02-15
ZHEJIANG WEIXING CRYSTAL
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Kaplan color crystal bead embryos are semi-finished products used to prepare Kaplan color crystal products. The existing Kaplan color crystal bead embryos are made in crucibles, which have poor coloring, spots, unstable product quality, low production efficiency, and are not suitable for Continuous mass production, in addition lead is harmful to the human body, and burning with coal causes environmental pollution

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] A kind of capland color crystal bead embryo of the present invention, the capland color crystal bead embryo is composed of the following components in parts by weight: 100 parts of quartz sand, 100 parts of fire powder, 80 parts of soda ash, 80 parts of broken glass, nitric acid 30 parts of sodium, 10 parts of borax decahydrate, 10 parts of calcium carbonate, 1 part of table salt, 10 parts of potassium nitrate, 0.1 part of cobalt oxide and 0.1 part of copper oxide.

[0019] The preparation process of the Kaplan color crystal bead embryo is as follows:

[0020] 1) Extract 100 parts by weight of quartz sand, 100 parts of fire powder, 80 parts of soda ash, 80 parts of broken glass, 30 parts of sodium nitrate, 10 parts of borax decahydrate, 10 parts of calcium carbonate, 1 part of table salt, and potassium nitrate 10 parts, 0.1 part of cobalt oxide and 0.1 part of copper oxide are mixed evenly;

[0021] 2) granulating the uniformly mixed Kaplan color crystal beads raw mate...

Embodiment 2

[0027] It differs from embodiment 1 in that this Capeland color crystal bead embryo is made up of the following parts by weight proportioning components: 250 parts of quartz sand, 250 parts of fire-throwing powder, 240 parts of soda ash, 300 parts of broken glass, 80 parts of sodium nitrate. parts, 50 parts of borax decahydrate, 45 parts of calcium carbonate, 15 parts of table salt, 40 parts of potassium nitrate, 1.5 parts of cobalt oxide and 3 parts of copper oxide.

Embodiment 3

[0029] It is different from embodiment 1 in that this Capeland color crystal bead embryo is made up of the following parts by weight proportioning components: 180 parts of quartz sand, 160 parts of fire-throwing powder, 150 parts of soda ash, 200 parts of broken glass, 60 parts of sodium nitrate. parts, 30 parts of borax decahydrate, 25 parts of calcium carbonate, 8 parts of table salt, 25 parts of potassium nitrate, 0.7 parts of cobalt oxide and 1.5 parts of copper oxide.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a capri blue crystal bead rough and a preparation method thereof. The capri blue crystal bead rough comprises the following components in parts by weight: 100-250 parts of quartz sand, 100-250 parts of fire-blasting powder, 80-240 parts of sodium carbonate, 80-300 parts of cullet, 30-80 parts of sodium nitrate, 10-50 parts of borax decahydrate, 10-45 parts of calcium carbonate, 1-15 parts of salt, 10-40 parts of potassium nitrate, 0.1-1.5 part of cobalt oxide and 0.1-3 parts of copper oxide. The cobalt oxide and copper oxide are adopted as coloring agents in the preparation process of the crystal bead rough, copper ions can better promote the reaction of raw materials, so that good coloring performance is obtained. The lead-containing raw materials are not adopted, so that the capri blue crystal bead rough is good in glossiness, bright in color, neat, colorless, free of spots, high in yield, free of lead and dust pollution, good in production benefit and capable of being produced in batches.

Description

technical field [0001] The invention relates to a Kaplan color crystal bead embryo and a preparation method thereof. Background technique [0002] The Capeland color crystal bead embryo is a semi-finished product used to prepare the Capeland color crystal product. The existing Capeland color crystal bead embryo process is made by crucible, which has poor coloring, spots, unstable product quality, low production efficiency, and is not suitable for Continuous mass production, and lead is harmful to the human body, and the use of coal to cause environmental pollution. SUMMARY OF THE INVENTION [0003] The technical problem to be solved by the present invention is to provide a Kaplan with good color reproducibility, consistent color, no color difference, no spots, no lead, no dust pollution, stable product quality, high production efficiency, and can be suitable for the production operation of continuous pool kiln. Color crystal beads. [0004] In order to solve the above-me...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C03C6/04C03C4/02C03B19/10C03C1/04
CPCC03C1/00C03B19/1005C03C1/04C03C4/0028C03C4/02
Inventor 杨鑫法杨建新
Owner ZHEJIANG WEIXING CRYSTAL
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products