Light porous artificial stone board and preparation method thereof
An artificial stone and stone slab technology, applied in the field of building materials, can solve the problems of low strength and heavy quality of artificial stone slabs, and achieve the effects of not easy weathering, light weight, and stable physical and chemical properties.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Embodiment 1 A kind of light porous artificial stone board
[0027] The density of the artificial stone board is 1.5g / cm 3 , There are 10,000 holes per cubic centimeter of artificial stone slab. Specifically, it is prepared by the following method:
[0028] (1) The composition of raw materials is: tile waste 40%; kaolin 45%, foaming agent (the foaming agent is composed of the following components by weight, sodium bicarbonate: carbon black: petroleum ether = 5:3:2) 0.5%, mineral sand 6.5%, glaze 8%; mix tile waste, kaolin, foaming agent, and put them into a ball mill for ball milling;
[0029] (2) Put the ball-milled raw materials into a ceramic press for dry pressing to obtain a green artificial stone slab;
[0030] (3) Put the artificial stone slab green body into a ceramic sintering furnace for sintering. The sintering conditions are: sintering at 450°C for 8 minutes, sintering at 750°C for 10 minutes, and sintering at 1250°C for 52 minutes; the cooked body is obt...
Embodiment 2
[0035] Embodiment 2 A kind of light porous artificial stone board
[0036] The density of the artificial stone board is 1.8g / cm 3 , Each cubic centimeter of artificial stone plate contains 3000 holes. Specifically, it is prepared by the following method:
[0037] (1) The composition of raw materials is: tile waste 36.5%; kaolin 50%, foaming agent (the foaming agent is composed of the following components by weight, sodium bicarbonate: carbon black: petroleum ether = 5:3:2) 0.5%, ore 8%, glaze 5%; mix tile waste, kaolin, foaming agent, and put them into a ball mill for ball milling;
[0038] (2) Put the ball-milled raw materials into a ceramic press for dry pressing to obtain a green artificial stone slab;
[0039] (3) Put the artificial stone slab green body into a ceramic sintering furnace for sintering. The sintering conditions are: sintering at 450°C for 8 minutes, sintering at 750°C for 10 minutes, and sintering at 1250°C for 52 minutes; the cooked body is obtained;
...
Embodiment 3
[0044] Embodiment 3 A kind of light porous artificial stone board
[0045] The density of the artificial stone board is 2.0g / cm 3 , Each cubic centimeter of artificial stone plate contains 3000 holes. Specifically, it is prepared by the following method:
[0046] (1) The composition of raw materials is: tile waste 35%; kaolin 49%, foaming agent (the foaming agent is composed of the following components by weight, sodium bicarbonate: carbon black: petroleum ether = 5:3:2) 1%, 5% mineral sand, 10% glaze; mix tile waste, kaolin, foaming agent, and put them into a ball mill for ball milling;
[0047] (2) Put the ball-milled raw materials into a ceramic press for dry pressing to obtain a green artificial stone slab;
[0048] (3) Put the artificial stone slab green body into a ceramic sintering furnace for sintering. The sintering conditions are: sintering at 450°C for 8 minutes, sintering at 750°C for 10 minutes, and sintering at 1250°C for 52 minutes; the cooked body is obtaine...
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com