Neodymium and antimony codoped stannic oxide nano-powder and preparation and application thereof
A technology of tin dioxide and nanopowder, which is applied in the direction of tin oxide, antimony oxide/antimony hydroxide/antimony oxyacid, and measuring devices, can solve the problem of low sensitivity of acetone gas and achieve excellent gas sensitivity, particle size The effect of small diameter and uniform particle size distribution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Take tin chloride, antimony chloride, neodymium nitrate and ethanol (the mol ratio of tin chloride and neodymium nitrate is 1:0.1; The mol ratio of tin chloride and ethanol is 1:40; The mol ratio of tin chloride and antimony chloride Molar ratio is 1:0.1), at first tin chloride is added in the ethanol, stirs to make it fully dissolve; Then add neodymium nitrate in this solution, stir to make it fully dissolve; Next antimony chloride is added in the above-mentioned ethanol solution, Stir to dissolve it, then raise the temperature of the solution to a certain temperature (70°C) and keep it for a period of time (1 hour), then adjust the pH to 7 by adding ammonia water to obtain a solid powder, which is centrifugally washed, dried and dried at a high temperature After calcining at 800°C for a certain period of time (1 hour), the neodymium-antimony co-doped tin dioxide can be obtained.
[0017] The powder prepared in this example is dispersedly coated on the gas sensor test ...
Embodiment 2
[0019] Take by weighing tin chloride, antimony chloride, neodymium nitrate and ethanol (the mol ratio of tin chloride and neodymium nitrate is 1:0.2; The mol ratio of tin chloride and ethanol is 1:50; The mol ratio of tin chloride and antimony chloride Molar ratio is 1:0.05), at first tin chloride is added in the ethanol, stirs to make it fully dissolve; Then add neodymium nitrate in this solution, stir to make it fully dissolve; Next antimony chloride is added in the above-mentioned ethanol solution, Stir to dissolve it, then raise the temperature of the solution to a certain temperature (80°C) and keep it for a period of time (2 hours), and then adjust the pH to 7 by adding ammonia water to obtain a solid powder, which is centrifugally washed, dried and dried at a high temperature After calcining at 700°C for a certain period of time (3 hours), the neodymium-antimony co-doped tin dioxide can be obtained.
[0020] The powder prepared in this example is dispersedly coated on t...
Embodiment 3
[0022] Take by weighing tin chloride, antimony chloride, neodymium nitrate and ethanol (the mol ratio of tin chloride and neodymium nitrate is 1:0.05; The mol ratio of tin chloride and ethanol is 1:60; The mol ratio of tin chloride and antimony chloride Molar ratio is 1:0.2), at first tin chloride is added in the ethanol, stirs to make it fully dissolve; Then add neodymium nitrate in this solution, stir to make it fully dissolve; Next antimony chloride is added in the above-mentioned ethanol solution, Stir to dissolve it, then raise the temperature of the solution to a certain temperature (60°C) and keep it for a period of time (0.5 hours), then adjust the pH to 7 by adding ammonia water to obtain a solid powder, which is centrifugally washed, dried and dried at high temperature After calcining at 900°C for a certain period of time (0.5 hours), the neodymium-antimony co-doped tin dioxide can be obtained.
[0023] The powder obtained in this example is dispersedly coated on the...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com