Anti-radiation anti-corrosion coating and preparation method thereof
An anti-corrosion coating and anti-radiation technology, applied in the field of coatings, can solve the problems of insufficient adhesion, insufficient function, difficult construction, etc., and achieve the effect of simple operation, easy realization and excellent anti-corrosion.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] Embodiment 1 of the present invention provides a radiation-proof and anti-corrosion coating, which includes the following raw materials in parts by weight: 10 parts of zirconium sol, 6 parts of aluminum dihydrogen phosphate, 8 parts of expanded graphite, 5 parts of carbon nanotubes, 1 part of titanium dioxide, glass 5 parts of powder, 5 parts of talcum powder, 10 parts of kaolin powder, 10 parts of wollastonite powder, 0.5 parts of hydroxypropyl methylcellulose, 1 part of dicyclopentenyloxyethyl acrylate and 20 parts of water, wherein, the implementation Each raw material in the example is industrial grade.
[0020] Preparation method: uniformly mix zirconium sol, aluminum dihydrogen phosphate, expanded graphite and water at 40°C to form the first mixed solution; add glass powder, talcum powder, wollastonite powder and kaolin powder to the second mixed solution One mixed solution, and ultrasonically dispersed for 30 minutes to obtain a second mixed solution; carbon nano...
Embodiment 2
[0022] Embodiment 2 of the present invention provides a radiation-proof and anti-corrosion coating, which includes the following raw materials in parts by weight: 11 parts of zirconium sol, 7 parts of aluminum dihydrogen phosphate, 9 parts of expanded graphite, 7 parts of carbon nanotubes, 2 parts of titanium dioxide, glass 6 parts of powder, 7 parts of talcum powder, 12 parts of kaolin powder, 11 parts of wollastonite powder, 1 part of hydroxypropyl methylcellulose, 2 parts of dicyclopentenyloxyethyl acrylate and 23 parts of water, wherein, the implementation Each raw material in the example is industrial grade.
[0023] Preparation method: uniformly mix zirconium sol, aluminum dihydrogen phosphate, expanded graphite and water at 50°C to form the first mixed solution; add glass powder, talcum powder, wollastonite powder and kaolin powder to the second mixed solution One mixed solution, and ultrasonically dispersed for 30 minutes to obtain a second mixed solution; carbon nanot...
Embodiment 3
[0025] Embodiment 3 of the present invention provides a radiation-proof and anti-corrosion coating, which includes the following raw materials in parts by weight: 12 parts of zirconium sol, 8 parts of aluminum dihydrogen phosphate, 10 parts of expanded graphite, 8 parts of carbon nanotubes, 3 parts of titanium dioxide, glass 7 parts of powder, 8 parts of talcum powder, 13 parts of kaolin powder, 13 parts of wollastonite powder, 1.5 parts of hydroxypropyl methylcellulose, 2 parts of dicyclopentenyloxyethyl acrylate and 25 parts of water, wherein, the implementation Each raw material in the example is industrial grade.
[0026] Preparation method: Under the condition of 60°C, uniformly mix zirconium sol, aluminum dihydrogen phosphate, expanded graphite and water to form the first mixed solution; add glass powder, kaolin powder, wollastonite powder and talc powder to the first mixed solution One mixed solution, and ultrasonically dispersed for 35 minutes to obtain a second mixed ...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com