Sintered hollow brick prepared from silt and dumped stone powder
A technology of waste stone powder and hollow bricks, applied in the field of building materials, can solve the problems of river silting, dust generation, air pollution, etc., and achieve the effects of reducing pollution, improving building functions, and saving energy.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A sintered hollow brick with silt waste stone powder, made of the following components by weight: 40% of silt, 25% of waste stone powder, 20% of coal gangue, 0.5% of plant straw powder, 3% of modified ceramic powder, 4% of sea mud, non Crystalline quartz particles 1.5%, sodium fluorosilicate 1.5%, kyanite 1%, polyvinyl alcohol resin 0.5%, sepiolite 1.5%, shell 1.5%;
[0032] The processing method of above-mentioned hollow brick is as follows:
[0033] (1) Crushing: The raw materials are crushed by fine crushing jaw crusher, hammer crushing or fine crushing roller machine. The diameter of raw material particles: 7% larger than 1.5mm, 18% larger than 1.5-0.9mm, 0.9-0.3mm 51%, 24% less than 0.3mm;
[0034] (2) Mixing and stirring: Add an appropriate amount of water to the crushed raw materials and stir evenly, and the moisture content of the mixed material after stirring is 12.5%; (Note: the above data is based on 500 grams per sample standard).
[0035] (3) Aging: put t...
Embodiment 2
[0052] A sintered hollow brick with silt waste stone powder, made of the following components by weight: 40% of silt, 25% of waste stone powder, 20% of coal gangue, 0.5% of plant straw powder, 3% of modified ceramic powder, 4% of sea mud, non Crystalline quartz particles 1.5%, sodium fluorosilicate 1.5%, kyanite 1%, polyvinyl alcohol resin 0.5%, sepiolite 1.5%, shell 1.5%;
[0053] The processing method of above-mentioned hollow brick is as follows:
[0054] (1) Crushing: The raw materials are crushed by fine crushing jaw crusher, hammer crushing or fine crushing roller machine. The diameter of raw material particles: 7% larger than 1.5mm, 18% larger than 1.5-0.9mm, 0.9-0.3mm 51%, 24% less than 0.3mm;
[0055] (2) Mixing and stirring: Add an appropriate amount of water to the crushed raw materials and stir evenly, and the moisture content of the mixed material after stirring is 12.5%; (Note: the above data is based on 500 grams per sample standard).
[0056] (3) Aging: put t...
PUM
Property | Measurement | Unit |
---|---|---|
Calorific value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com