A clothing and fur technology, applied in clothing, clothing, protective clothing, etc., can solve the problems of wrinkles and snags, difficult sewing, and affect the appearance, so as to increase the strength and appearance of clothing, better wearing experience, and convenient cutting sewing effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A preparation method for fur clothing comprises the following steps: connecting multiple pieces of tanned animal furs by sewing to obtain large pieces of animal furs, coating the reverse side of the animal furs with an adhesive, pasting a knitted inner lining, and heating at 50°C for 8 Minutes, cut and sew the finished garment, sew the knitted belt at the joint of the garment, wash it with an organic solvent at room temperature for 5 minutes, and dry it at 30°C for 8 minutes to obtain a fur garment;
[0019] In this embodiment, the adhesive consists of the following components: 100 g of methyl acrylate, 2 g of azobisisobutyronitrile, 8 g of sodium dodecylsulfonate, plasticizer bis(2-ethylhexyl) phthalate Ester 10g, 20g toluene and 20g carbon tetrachloride composition.
[0020] The organic solvent consisted of 48g acetone and 72g dichloromethane.
Embodiment 2
[0022] A preparation method for fur clothing comprises the following steps: connecting multiple pieces of tanned animal furs by sewing to obtain large pieces of animal furs, coating the reverse side of the animal furs with an adhesive, pasting a knitted inner lining, and heating at 55°C for 5 Minutes, cut and sew the finished garment, sew the knitting belt at the joint of the garment, wash it with an organic solvent at room temperature for 8 minutes, and dry it at 40°C for 5 minutes to obtain a fur garment;
[0023] In this embodiment, the adhesive consists of the following components: 100g of methyl acrylate, 1g of azobisisobutyronitrile, 9g of sodium dodecylsulfonate, 12g of plasticizer dibutyl phthalate, 12g of toluene and 24g carbon tetrachloride composition.
[0024] The organic solvent consisted of 43.5 g acetone and 78.5 g dichloromethane.
Embodiment 3
[0026] A preparation method for fur garments comprises the following steps: connecting several pieces of tanned animal furs by sewing to obtain large pieces of animal furs, coating the reverse side of the animal furs with an adhesive, pasting a knitted inner lining, and heating at 60°C for 3 Minutes, cut and sew the finished garment, sew the knitting belt at the joint of the garment, wash it with an organic solvent at room temperature for 10 minutes, and dry it at 50°C for 3 minutes to obtain a fur garment;
[0027] In this embodiment, the adhesive is composed of the following components: 100g of methyl acrylate, 3g of azobisisobutyronitrile, 10g of sodium dodecylsulfonate, 15g of plasticizer tricresyl phosphate, 8g of toluene and 24g of tetrachloro carbon composition.
[0028] The organic solvent consisted of 43g acetone and 85g dichloromethane.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com