An adhesive and carton technology, applied in the direction of adhesive types, starch-derived adhesives, non-polymer adhesive additives, etc., can solve the problems of unreliable quality, slow drying speed, and high production costs, reaching The effect of improving oxidation effect, excellent adhesion performance, and improving initial adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Example 1: At room temperature, mix 25kg of cornstarch with 50kg of water, slowly add and stir until milky white starch slurry is obtained, and 8kg of sodium hydroxide is prepared into a certain concentration of sodium hydroxide solution and slowly added to the starch slurry , to obtain pre-gelatinized milky white viscous starch paste; then take 0.08kg of potassium permanganate and 0.24kg of phosphoric acid, use hot water to prepare a certain concentration of composite oxidant solution, add in the above-mentioned starch paste; then take 0.12kg of boric acid and heat Dissolve in water to form a solution with a certain concentration and add starch paste to form a glue. Finally, take 0.3 kg of nano sepiolite powder and add it to the glue to finally obtain an oxidized starch adhesive. Stir the adhesive continuously and then slowly add 0.15 kg of alum solution to form a glue. Get the finished product.
Embodiment 2
[0017] Example 2: At room temperature, mix 30kg of cornstarch with 55kg of water, slowly add and stir until milky white starch slurry is obtained, and take 10kg of sodium hydroxide to prepare a certain concentration of sodium hydroxide solution and slowly add it to the starch slurry , to obtain pre-gelatinized milky white viscous starch paste; then take 0.04kg of potassium permanganate and 0.28kg of nitric acid to prepare a certain concentration of composite oxidant with hot water, and add it to the above-mentioned starch paste; then take 0.16kg of boric acid and dissolve it in hot water Make a solution with a certain concentration and add starch paste to form a glue solution. Finally, take 0.45kg of nano-sepiolite powder and add it to the glue solution, and then slowly add electricity to finally obtain an oxidized starch adhesive. Stir the adhesive continuously and then slowly add alum The solution is 0.25kg, and the finished product is finally obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com