A technology of diatom mud and quartz stone, which is applied in the field of artificial building materials preparation, can solve problems such as human health and living environment hazards, unfavorable quality of life, disrupting economic order, etc., and achieves low execution difficulty, simple production process, and improved use quality Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] A quartz stone containing diatom mud, including main materials and auxiliary materials,
[0033] The main ingredients include 12 parts of diatom mud, 1 part of tortoise shell, 75 parts of 30-120 mesh quartz sand, 40 parts of 300-700 mesh quartz powder, 1 part of obsidian powder, 1 part of synthetic resin, 1 part of synthetic rubber, polyacrylate 2 copies;
[0034] The auxiliary materials include 0.3 parts of titanate coupling agent, 0.1 parts of ethylene triamine, 0.1 part of diethylene triamine, 0.1 part of jute, 0.2 parts of glass cloth, 0.2 parts of coloring material, 0.1 part of rock wool board powder and 0.4 parts of additives ;
[0035] The raw materials of additives include paraffin oil, methyl silicone oil, glycerin, polyvinyl acetate, α-ethyl cyanoacrylate and linear low density polyethylene, paraffin oil, methyl silicone oil, glycerin, polyvinyl acetate, α-cyanoacrylate The mass ratio of ethyl acrylate to linear low density polyethylene is 4:3:1:2:0.5:0.3. ...
Embodiment 2
[0050] A quartz stone containing diatom mud, including main materials and auxiliary materials,
[0051] The main ingredients include 15 parts of diatom mud, 3 parts of tortoise shell, 90 parts of 30-120 mesh quartz sand, 45 parts of 300-700 mesh quartz powder, 4 parts of obsidian powder, 4 parts of synthetic resin, 4 parts of synthetic rubber, polyacrylate 6 copies;
[0052] The auxiliary materials include 1 part of titanate coupling agent, 0.5 part of ethylene triamine, 0.6 part of diethylene triamine, 0.5 part of jute, 0.7 part of broken glass cloth, 0.7 part of colorant, 0.5 part of rock wool board powder and 0.9 part of additive ;
[0053] The raw materials of additives include paraffin oil, methyl silicone oil, glycerin, polyvinyl acetate, α-ethyl cyanoacrylate and linear low density polyethylene, paraffin oil, methyl silicone oil, glycerin, polyvinyl acetate, α-cyanoacrylate The mass ratio of ethyl acrylate to linear low density polyethylene is 4:3:1:2:0.5:0.3.
[005...
Embodiment 3
[0068] A quartz stone containing diatom mud, including main materials and auxiliary materials,
[0069] The main ingredients include 13 parts of diatom mud, 2 parts of tortoise shell, 85 parts of 30-120 mesh quartz sand, 42 parts of 300-700 mesh quartz powder, 2 parts of obsidian powder, 2 parts of synthetic resin, 2 parts of synthetic rubber, polyacrylate 3 copies;
[0070] The auxiliary materials include 0.7 parts of titanate coupling agent, 0.3 parts of ethylene triamine, 0.4 parts of diethylene triamine, 0.3 parts of jute, 0.5 parts of glass cloth scraps, 0.3 parts of colorants, 0.4 parts of rock wool board powder and 0.7 parts of additives ;
[0071] The raw materials of additives include paraffin oil, methyl silicone oil, glycerin, polyvinyl acetate, α-ethyl cyanoacrylate and linear low density polyethylene, paraffin oil, methyl silicone oil, glycerin, polyvinyl acetate, α-cyanoacrylate The mass ratio of ethyl acrylate to linear low density polyethylene is 4:3:1:2:0.5:...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com